Cheap Potassium Iodide


I just ran across some cheap potassium iodide and thought people might be interested: https://www.ebay.com/itm/100g-3-52oz-Pure-Potassium-Iodide-C...



View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 31-8-2018 at 01:02
Thanks


Even though I still have c50g I could not resist buying 100g at that price.

... stock up, be ready for the next nuclear event .......... :P




For similar reasons I also have excess stock of iodine prills.
... I now need to do lots of iodine based chemistry ... :P
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 31-8-2018 at 01:54


I considered buying a kilogram but placed a small order for only 500 grams instead. Potassium iodide is expensive... 500 grams is only about 3 moles. Still, that's one of the best prices I've seen.





View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 31-8-2018 at 05:03


bought 100g just for the price, at the moment i don't have to use it




---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
highpower48
Hazard to Self
**




Posts: 98
Registered: 30-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2018 at 07:09


Only problem I see is a 98% seller rating. I just got burned on an order of resistors. This is the first time that I was attempted to be scammed on eBay. I did recieve my money back, through eBay. But now I have to find another dealer who has 5watt resistors and reorder. The bad dealer had a rating of 99.3%.

I would love to get a couple of 100 grams of potassium iodide to make elemental iodide but this one seems just to good to be true.
View user's profile View All Posts By User
CobaltChloride
Hazard to Others
***




Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline


[*] posted on 31-8-2018 at 07:21


I bought some KI from such a seller on eBay and the chemical didn't have any problems. I bought my 100g of KI from here: https://www.ebay.com/itm/100g-3-52oz-Pure-Potassium-Iodide-C...

It doesn't seem to contain any other halogens besides iodine. I combined a bit of the KI and some oxone (in excess) in a test tube, added a bit of water and I didn't get any brown or yellow-green fumes, just some black solid and a bit of purple vapor afterwards.

The only problem with this KI is that it is slightly wet and sticks to its container. This can be solved by putting the KI in a dessicator for a few days.
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 31-8-2018 at 08:01


Quote: Originally posted by CobaltChloride  
I bought some KI from such a seller on eBay and the chemical didn't have any problems. I bought my 100g of KI from here: https://www.ebay.com/itm/100g-3-52oz-Pure-Potassium-Iodide-C...

It doesn't seem to contain any other halogens besides iodine. I combined a bit of the KI and some oxone (in excess) in a test tube, added a bit of water and I didn't get any brown or yellow-green fumes, just some black solid and a bit of purple vapor afterwards.

The only problem with this KI is that it is slightly wet and sticks to its container. This can be solved by putting the KI in a dessicator for a few days.


Now that is a good price. I plan on testing mine when it arrives, and I will of course demand my money back if it isn't reasonably good quality.




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 31-8-2018 at 10:30


Some time ago, I ordered 300 grams of this seller and I am happy with the stuff. For just over EUR 15 I have 300 grams of decent quality KI, which is a very good price.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
happyfooddance
National Hazard
****




Posts: 530
Registered: 9-11-2017
Location: Los Angeles, Ca.
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2018 at 16:27


Shipping says estimated 6 weeks :(
View user's profile View All Posts By User
Tdep
National Hazard
****




Posts: 516
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline

Mood: PhD is done! It isn't good but it's over lol

[*] posted on 31-8-2018 at 19:15


I might grab some too, good link thanks. But yeah, good thing I don't want it urgently, the shipping estimate to Aus is 7-12 weeks wow
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 3-9-2018 at 00:42


Oh yes, shipping takes a loooooooong time. Just order it now and slooooowly think of any nice experiments you will do with it when it arrives ;)



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 13-9-2018 at 04:26
Received today, 95g KI


The KI arrived this morning, it looked a little damp and felt underweight.
The KI that arrived weighed 95.55g but actually weighed 95.07g after drying,.
5% underweight... OK for the price if it is pure KI ... tbd.
View user's profile View All Posts By User
Tdep
National Hazard
****




Posts: 516
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline

Mood: PhD is done! It isn't good but it's over lol

[*] posted on 26-11-2018 at 02:23


So I ordered some of this potassium iodide. Its only $6!
It took a while to turn up. And when it did arrive, it is completely unlabelled. Sure fine, it was free shipping.
Its got some yellow spots through it. Faint, but they're there. Fine, that's okay, i'll do a recryst, it was only $6.
It also has a mild unpleasant smell. Very mild, but its there. Whatever, it'll come out in the recryst.
Have I put up with too much? Well, this is where I draw the line: it isn't even potassium iodide. Now that's not fine, even if it was only $6!

I'm trying to titrate my ozone generator. Get out the new KI, make a standard solution, run it.... nothing. Add some other (more expensive) NaI... instant reaction! Do it some more, run the ozone through a conc solution of the new, now unknown salt.... nothing. I can say with complete confidence that I have been sold a highly soluble salt that does NOT contain the iodide ion in any concentration.
Looking at it now I can feel it is not dense enough.
Oh well, guess I only tipped $6 down the drain....
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 26-11-2018 at 02:37


I forgot to report back on this. I also ordered from this listing. I tried to use this new KI for peroxide testing of ethers but I didn't get any reaction to my hydrogen peroxide control sample. I tried the exact same technique with known-good KI and it worked fine.
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 26-11-2018 at 03:03


I never actually got mine... they canceled my order and refunded my money.



View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 26-11-2018 at 05:19


well, i got mine and did not test it, if many here received something other than iodide i should really test it



[Edited on 26-11-2018 by Ubya]





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 26-11-2018 at 05:39


This is sad to read. I ordered 300 grams from this seller (or a similar one, that may be the catch) and I had good experience with it (like CobaltChloride). I tested it immediately on arrival by taking some of the salt, dissolving it in dilute HCl and added a little 10% H2O2. I immediately got a grey precipitate of iodine in this reaction. So, apparently the sellers have different batches, some of them being OK, others not OK. This is the risk of buying cheap stuff from China. Up to now I have been lucky with chems from China, with electronics I once had inferior components, with lower gain and inferior parameters (e.g. transistors with low beta-factor and higher than tolerated resistance).

Half a year ago I also purchased 250 grams of elemental iodine from China for a little over EUR 20 with free shipping. I received it in a plastic brown bag, which was wrapped in another vacuum sealed bag, made of laminated plastic/aluminium. The iodine was fine though, I rebottled it. It leaves no residue on strong heating.

If you don't get what you pay for you either get a refund from the seller, or from eBay.

JJay's link and CobaltChloride's link are different. Could that be the difference in experiences?

[Edited on 26-11-18 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 26-11-2018 at 05:55


Quote: Originally posted by woelen  

If you don't get what you pay for you either get a refund from the seller, or from eBay.

JJay's link and CobaltChloride's link are different. Could that be the difference in experiences?


To clarify I ordered from JJay's link.

The problem with getting refunds is that often when it arrives from China after a couple of months, I don't have time to test it right away, so by the time I realise it's fake, it's too late.

View user's profile View All Posts By User
Loptr
International Hazard
*****




Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline

Mood: Grateful

[*] posted on 26-11-2018 at 06:07


I also ordered from JJay's link and received my order fairly quickly. This was very early on, about as soon as I saw this thread. I just stowed it away in the back of my cabinet, but now I am thinking I need to test it.



"Question everything generally thought to be obvious." - Dieter Rams
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 26-11-2018 at 06:29


I have just returned from my lab after quickly testing a sample of my 100g ... pass

Solubility was indistinguishable from a known good sample, side-by-side.
I diluted the two samples then adding drops of silver nitrate solution alternately to each sample produced similar light yellow 'clouds'
If it is not KI then it is an excellent fake.
I've not tested the purity.

EDIT: Yes, I am dumb ... after reading posts below I realiseded that even sodium chloride would give a similar result.
I'll try to test it properly tomorrow.

[Edited on 27-11-2018 by Sulaiman]




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 26-11-2018 at 09:56


I just tested mine again:

  1. Flame colour reveals definite presence of sodium.
  2. Dissolution of a spatula full in 15ml UP water, acidification with a small amount of HNO3, and addition of 1ml 0.1N AgNO3 gives a white precipitate. This precipitate dissolves on addition of a few ml of conc. NH3


So. I've been sent some expensive table salt.
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 26-11-2018 at 13:33


I would be furious. Sorry about that; I just thought the price was really good. Definitely request a refund....





View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 26-11-2018 at 14:49


i'm really mad, it's not iodide, and it's not even a potassium salt, just sodium, most probably just fking table salt...
man i'm mad. fuck





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 26-11-2018 at 15:00


I’m guessing that y’all got sent iodized salt, at best.

[Edited on 11-26-2018 by WGTR]




View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 26-11-2018 at 16:17


Definitely contact eBay and/or the seller and complain. I don't know the seller and am not affiliated with them in any way (and they refunded my money), but if they are scamming people, they should be required to make amends and stop.



View user's profile View All Posts By User