Ground glass valves freezing
I find that the T-joints on my Gregar extractor freeze during use and I can't turn them (sometimes for example it's useful to drain the
upper section by opening the bottom valve, to prevent the thimble overflowing due to clogging by too fine particles; draining makes more gravity push
on the solvent column in the thimble).
I can't see how I can put Teflon tape as I do on the joints, without making the valves leak. What's the standard procedure? I've read
about greasing with glycerin etc., but that doesn't work with solvents such as acetone etc. or HNO3 extraction.
\"One of the surest signs of Conrad\'s genius is that women dislike his books.\" --George Orwell
|
|
mick
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 338
Registered: 3-10-2003
Member Is Offline
Mood: No Mood
|
|
You could try lapping it in.The old glass taps were sold as a matching pair. Good quality fine wet or dry wrapped around the barrel with WD40 might
get a better fit. A smear of silicone grease should survive vacuum and organic solvents for a few months.
mick
|
|
Thermal
Harmless
Posts: 41
Registered: 31-1-2004
Member Is Offline
Mood: No Mood
|
|
I'd go with fine valve lapping compound (as in engine cylinder head valves) rather than the sandpaper. Maybe some jewelers rouge.
I'd also second the silcone grease.
If they get really stuck I find the heatgun rarely fails to get ground glass joints to part ways.
|
|
Quince
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 773
Registered: 31-1-2005
Location: Vancouver, BC
Member Is Offline
Mood: No Mood
|
|
I ended up using a torch until the sulfur melted, and a few whacks with a mallet to get it out. I'm never putting sulfur in this again, what a
pain to clean out...I had to scrub the outside of my glassware with steel wool to get it all off.
[Edited on 3-10-2005 by Quince]
\"One of the surest signs of Conrad\'s genius is that women dislike his books.\" --George Orwell
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
Nitric acid will work for this purpose. It oxidizes sulfur to sulfuric acid, removing it as an aqueous
H<sub>2</sub>SO<sub>4</sub> solution.
|
|
DrP
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 625
Registered: 28-9-2005
Member Is Offline
Mood: exothermic
|
|
Silicone greese is excellant for glass joints - inert and hold very goog vacuum.
|
|
silonyl
Harmless
Posts: 23
Registered: 18-7-2005
Member Is Offline
Mood: No Mood
|
|
grease is definitely the way to go. Silicone will be fine if you don't run into high-temps and expecially highly reactive conditions.
When silicond doesn't cut it, there are greases made by Apiezon (spelling probably off) that have excellent resistance to both heat and chemical
attack. I think back on both H and M types working quite happily.
.s
|
|
Quince
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 773
Registered: 31-1-2005
Location: Vancouver, BC
Member Is Offline
Mood: No Mood
|
|
Can someone suggest the most common things that silicone is NOT good for?
I have a spray can of "Heavy Duty Silicone Multi-use lubricant" and I'm wondering if it's usable. It says it contains heptane,
propane-isobutane, and dimethylpolysiloxane. I guess the first two are propellants, and the last is the silicone.
Also, how do you remove it afterward?
[Edited on 10-10-2005 by Quince]
\"One of the surest signs of Conrad\'s genius is that women dislike his books.\" --George Orwell
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Quote: | Originally posted by Quince
Also, how do you remove it afterward?
|
As I recall, that's a very good question, which is one of the reasons silicone oils are weary to use.
Tim
|
|
DrP
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 625
Registered: 28-9-2005
Member Is Offline
Mood: exothermic
|
|
Buy a tube of silicone grease. Don't ust too much on the joint and just put it round the top. Wipe it off afterwards with some tissue wipe.
Bet you'll be fine with this. Silicone grease is quite expensive though.
|
|
Quince
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 773
Registered: 31-1-2005
Location: Vancouver, BC
Member Is Offline
Mood: No Mood
|
|
Hmm, it doesn't seem to just "wipe off".
\"One of the surest signs of Conrad\'s genius is that women dislike his books.\" --George Orwell
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Fine, if you're worried about the 3 microgram residue left behind...carefully burn it in a bunsen flame and wipe off the SiO2 with a bit of
sandpaper. Satisfied?
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
Quince
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 773
Registered: 31-1-2005
Location: Vancouver, BC
Member Is Offline
Mood: No Mood
|
|
Er, I thought glass was mostly SiO2 also.
\"One of the surest signs of Conrad\'s genius is that women dislike his books.\" --George Orwell
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
I think vulture was being sarcastic.
|
|
Quince
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 773
Registered: 31-1-2005
Location: Vancouver, BC
Member Is Offline
Mood: No Mood
|
|
Oh... but to what end?
\"One of the surest signs of Conrad\'s genius is that women dislike his books.\" --George Orwell
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Silicones burn with a yellow flame (at least the last polymerized acetic polysilicone I burned), leaving a large amount of white ash, silica fume.
I would imagine the residue would wipe off, rather than requiring sand paper, but I could be wrong.
Tim
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
12AX7 is right and I wasn't being sarcastic. If high enough temperatures are applied, silicone will burn leaving very pure SiO2. Sometimes it
will cake or widen the joint in which case it wont fit anymore and that's when you need sandpaper.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
Does sandpaper damage the joint in this case?
I assume the cooling must be done carefully to avoid cracking?
|
|
trilobite
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 152
Registered: 25-2-2004
Location: The Palaeozoic Ocean
Member Is Offline
Mood: lonely
|
|
The commercial product used in glass stopcocks, dessicator flanges etc is usually called stopcock grease, but I've also seen the German word
Exsikatorfett (dessicator grease) used for it. The last variety I ran into was advertised not to contain silicon, it was thick and sticky grease
obviously of very high boiling point. The question that interests me is where is such grease used outside laboratory (OTC acquisition), but I
haven't looked into it. It's a very useful product. The typical silicone grease works but it is not as thick and not as good. Here is a link
about these products.
http://www.sas.org/E-Bulletin/2002-09-20/labNotesCoyne/body....
|
|
Quince
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 773
Registered: 31-1-2005
Location: Vancouver, BC
Member Is Offline
Mood: No Mood
|
|
According to this link, silicone grease should not be used with vacuum as it deposits a film on the inside of the glassware; in heat it burns
completely into the glass, and the removal method given is soaking in a base. Overall, pretty nasty! Given the problems with removal of the
fluorinated grease as well, I guess PTFE sleeves or tape remain the best option in most cases.
[Edited on 16-10-2005 by Quince]
\"One of the surest signs of Conrad\'s genius is that women dislike his books.\" --George Orwell
|
|