crystal structure of 2D pillared copper phosphonate MOF
Hey guys I am uploading an image from the crystal structure of a MOF i made. Thought I will not go into much details since it is still not published .
Enjoy ![:)](./images/smilies/smile.gif)
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Online
Mood: No Mood
|
|
At the risk of looking stupid, what does MOF stand for?
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Metal-organic framework
|
|
DrP
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 625
Registered: 28-9-2005
Member Is Offline
Mood: exothermic
|
|
Superb - I only recently read about them a few months back. There must be so much work to be done with them trying different metals/organics to see
what material properties result.
Really exciting material.
\"It\'s a man\'s obligation to stick his boneration in a women\'s separation; this sort of penetration will increase the population of the younger
generation\" - Eric Cartman
|
|
Zool
Harmless
Posts: 18
Registered: 6-1-2017
Member Is Offline
Mood: No Mood
|
|
And relatively easy to make . Quantum mechanics does all the work for you and so small molecules and ions they self asseble to create bigger and more
complex structures. Viva la quantum mechanica !!!
|
|