Author: Subject: Looking for a UK source of aluminium granules for a heat bath
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 8-3-2018 at 16:33
Looking for a UK source of aluminium granules for a heat bath


I've seen mentions on this site of using aluminium granules/shot/pellets in a heat bath as a replacement for oil, sand, water, etc. I'd quite like to try this but I'm having issues finding suitable aluminium shot in the UK. Got any ideas?
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 8-3-2018 at 17:33


It's a bit expensive, but airsoft players use solid Aluminum 6mm balls for their "sniper rifles".

https://m.ebay.com/itm/1000-RD-New-Aluminum-Metal-3g-0-30g-6...

View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2542
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 8-3-2018 at 20:40


It might be possible to make your own if you have a furnace that can melt aluminum (660 °C). See: https://en.wikipedia.org/wiki/Shot_(pellet)#Manufacture

[Edited on 3-9-2018 by Metacelsus]




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 9-3-2018 at 04:47


I've seen the aluminium airsoft pellets but like you say that would be pretty pricey to buy enough.

Unfortunately I don't have the facilities to melt aluminium.
View user's profile View All Posts By User
yobbo II
National Hazard
****




Posts: 766
Registered: 28-3-2016
Member Is Offline

Mood: No Mood

[*] posted on 9-3-2018 at 06:29



Try cooking shops. I have seen pellets for sale used for putting into pastry molds (the things you would put jam into when cooked ) to keep them in shape when they are being baked. Also called pie weights.

Yob
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 9-3-2018 at 07:38


I briefly considered making my own, if you have some time on your hands and access to scraps of the Aluminum power cable used for mains electric supply, you might source cable scraps from a metal recycling company or an electrical installer?

The individual strands of conductor inside the cable are soft, pure Aluminum and very easy to shear. If one were to strip out and unwind several pounds of these Aluminum conductors and more or less straighten them out, one could feed several at a time through a sheet metal shears with the material stop set just about 1 diameter of the individual strand, producing little cylinders about as long as wide.

Once you had enough of these pellets, you could tumble them in a ball mill (rock polisher!) until the cut ends were well rounded, or possibly just use them as they came out of the shears if the sharp cut ends were not objectionable.

20180309_093517.png - 1.5MB
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 10-3-2018 at 10:41


Hmm that sounds like a lot of work, I was kinda hoping for an off the shelf solution...
View user's profile View All Posts By User
yobbo II
National Hazard
****




Posts: 766
Registered: 28-3-2016
Member Is Offline

Mood: No Mood

[*] posted on 10-3-2018 at 15:34


AAAAAAAAAAAAAaaaaaaaaaa no it would not!!

Would copper do the same job just as good. Easier to obtain the cable too.

Yob

[Edited on 10-3-2018 by yobbo II]
View user's profile View All Posts By User
LearnedAmateur
National Hazard
****




Posts: 513
Registered: 30-3-2017
Location: Somewhere in the UK
Member Is Offline

Mood: Free Radical

[*] posted on 11-3-2018 at 06:05


Copper would be even better in fact, higher thermal conductivity and lower heat capacity, meaning it takes less energy to reach a higher temperature.



In chemistry, sometimes the solution is the problem.

It’s been a while, but I’m not dead! Updated 7/1/2020. Shout out to Aga, we got along well.
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 11-3-2018 at 06:16


True, but copper has roughly 3 times the density of aluminium, and it's more expensive per unit mass. So a copper granule bath is going to be more expensive.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3738
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 11-3-2018 at 06:20


Copper would give a lot of 'bouyancy' as it is quite dense.
Perfect spheres conduct heat poorly,
shapes more like a water drop on plastic would still be smooth but conduct heat better,
- very oblate spheroids.

I hope that you find a suitable medium for high temperatures as I'm going there soon.

What temperatures do you wish to operate at ?
(e.g. infra-red or hot-air can boil Az. H2SO4, mantles can heat to near glass m.p.)




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 11-3-2018 at 06:42


I won't be routinely doing anything above around 200c, on occasion might go up to the BP of azeotropic sulphuric acid. I want something for general use which is less messy than oil (and less hazardous re accidental introduction of drops of water) and has better thermal conductivity than sand. Preferably reasonably cheap too...

Aluminium (and other metals) in powder form is relatively easy to get but that would be messy and possibly an inhalation hazard depending on particle size.



[Edited on 12-3-2018 by DavidJR]
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 11-3-2018 at 06:42


Quote: Originally posted by DavidJR  
I'm having issues finding suitable aluminium shot in the UK. Got any ideas?


Perhaps you could look OUTSIDE the UK, if none are to be found and you do not have the time to make your own.

Or you could call a few metal salvage/recycling businesses and ask if they receive Aluminum punch press scrap such as this.

s-l400-1.jpg - 19kB s-l400.jpg - 14kB
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 11-3-2018 at 06:49


"Shipping: Does not ship to United Kingdom"
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 11-3-2018 at 06:54


I have emailed this company: http://www.lowdenlimited.co.uk/PureMetals/Aluminium.html but yet to receive a reply.
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 11-3-2018 at 08:08


BTW are there BB guns in Britain? 2 kg of copper coated steel .177 caliber shot goes for $8.49 with free shipping on USA amazon.



"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 11-3-2018 at 08:53


Steel is much less thermally conductive than aluminium or copper, and as mentioned above perfect spheres aren't great for heat transfer either.

edit:

Though I suppose the real question is would steel work anyway?
You can get steel bead blasting media for cheaper than that, and some types are irregular rather than perfectly spherical.

[Edited on 11-3-2018 by DavidJR]
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1331
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 11-3-2018 at 12:44


Have you tried a machine shop? They may have aluminium swarf you can try for free.



Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 12-3-2018 at 09:33


Got a response from Lowden Limited, they have quoted £54 per kilo excl vat and shipping. Eek! Perhaps not.

I also contacted Guyson, who manufactures/sells shot blasting equipment and media, and they have quoted about £310 incl shipping for a 25kg bag of their Alusad A16 aluminium granules. That is a more reasonable £12.40 per kilo but I really don't need 25kg so unless anyone wants to group buy then that's a no-go.

[Edited on 12-3-2018 by DavidJR]
View user's profile View All Posts By User
yobbo II
National Hazard
****




Posts: 766
Registered: 28-3-2016
Member Is Offline

Mood: No Mood

[*] posted on 2-4-2018 at 13:49



If you were to get some Al drink cans and cut into small squares using a scissors, or perhaps cut lots of strips, curl the strips and them cut to give each square a three dimensional lift.

Getto
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3738
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 2-4-2018 at 16:53


At those costs it is worth buying a heating mantle.
I use one of these https://www.ebay.co.uk/itm/500ML-250W-Hand-Woven-Adjustable-...
one of these https://www.ebay.co.uk/itm/New-4000W-AC-220V-SCR-Voltage-Reg...
and a tin can.
Less than £10 total.
(magnetic stirring still under development :)




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 2-4-2018 at 18:09


If anything is to be cut, it should be rod such as from hardware stores here.



"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 3-4-2018 at 14:43


Quote: Originally posted by Sulaiman  
At those costs it is worth buying a heating mantle.
I use one of these https://www.ebay.co.uk/itm/500ML-250W-Hand-Woven-Adjustable-...
one of these https://www.ebay.co.uk/itm/New-4000W-AC-220V-SCR-Voltage-Reg...
and a tin can.
Less than £10 total.
(magnetic stirring still under development :)


You know what, that's not a bad idea...
View user's profile View All Posts By User