Nituff® coatings
What's the process for treating metals with this type of hardcoat?
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Hm, is that nitriding? Not sure, I think it involves plasma in a low pressure chamber.
Tim
|
|
FrankRizzo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 203
Registered: 9-2-2004
Member Is Offline
Mood: No Mood
|
|
It's a hard coat anodizing process that impregnates the layer with PTFE and a black dye of some sort.
Rich Wolter offers some star pumps (pyro) with the coating and the stuff is practically unscratchable.
|
|
Cyrus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 397
Registered: 24-4-2004
Location: Ancient Persia
Member Is Offline
Mood: No Mood
|
|
Is the base metal aluminum? Of course, when that's anodized the final layer has sort of hollow tubules that can be filled with dyes, and then
closed off somehow, by boiling them or reacting them with a nickel salt, IIRC. There are plenty of good pages on Al anodizing.
So the black dye seems explainable, although I'm not sure why it's put there. Perhaps the hollow tubules are filled with a product similar
to the Du Pont teflon spray mentioned recently in a different thread (about teflon, I think). That would be a cool coating!
|
|
FrankRizzo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 203
Registered: 9-2-2004
Member Is Offline
Mood: No Mood
|
|
Cyrus,
Yes, the base metal has to be Aluminum. I'm familiar anodizing dyes and the process, but this appears to be a more involved procedure. The
porous AlO3 layer is somehow impregnated with sintered PTFE.
We can speculate all day based on the description of the final product, but the procedure is a trade secret which I'd like to find out. :-)
http://www.techsavvy.com/industry/file/national/08qxf/nim06....