Laboratory of Liptakov
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1367
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
Wrappolite
![wrappolite.jpg - 341kB](http://www.sciencemadness.org/talk/files.php?pid=503742&aid=64089)
Here I am trying to introduce some invention of prof. Liptakov. The basic idea is two aluminum foils that seal hermetically the energy material
inside. Aluminum foil fulfills 3 basic functions. 1) Handling carrier film, 2) secondary fuel 3) moisture barrier. But also against evaporation,
depending on the type of EM inside. The basic design is 2 Alu foils of 0.05 mm thick. Between their are AN crystals + EG in stechiomeric ratio. Foil
and grain create air pockets that are important for proper function. During roll-up in the form of a condenser, additional air pockets are formed
between the outer sides of the foil. This ensures that the low density is maintained during scrolling. Usually in the shape of a thick cylinder. Foil
tape is possible easy divide for right weight of use. Or easily to edit to cube shape or rectangle. Or any shape without loss of properties. Within a
certain range of density, of course.
EM inside can be also almost anything that evaporates or is liquid. Alu foil fully replaces fine aluminum powder. Therefore, the foil is counted in
the oxygen balance.
The exact details of the ratios, manufacturing process and all the possibilities of use will not be given for understandable reasons.
Dr......
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
In my experience, Aluminum foils are very easily pierced, torn or just develop pin holes where they have been bent.
When wrapping up the item, how do.you deal with either the interior foil (tighter curve) from becoming corrugated and leaking, or the outer foil (must
cover longer distance) from tearing?
Agree on the foil becoming part of the fuel or even providing a thermobaric effect for any reasonably hot, brissant explosive filling-
IT'S THE JELLY ROLL OF DEATH!!!
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Laboratory of Liptakov
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1367
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
During rolling to shape capacitor arises more air gaps on insides layer. EG works as oil. Better is always roll on bigger basic start diameter from 4
cm. At thickness 0,5 mm / 40mm Is effect dilatation between inside and outside Alu foil small. Of course, that someplace arises piercing points.
But if is grains under 0,2 mm, is piercing almost nothing. It s not some proffesional device. But works from No. 8. Always.
Thermobaric effect ? Of course. Also Always .............
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
roXefeller
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 463
Registered: 9-9-2013
Location: 13 Colonies
Member Is Offline
Mood: 220 221 whatever it takes
|
|
Do you have any experience with critical diameter? I wonder if it has application as det cord. I know its almost untenable though.
[Edited on 15-1-2018 by roXefeller]
|
|
Laboratory of Liptakov
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1367
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
Minimal 3 cm diameter is condition. Maybe as thick detcord should by works. With AN - EG. But 1 meter long charge it was not tried.
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Microtek
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 849
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
A member here on SM (I don't remember who, exactly) experimented with thermobaric devices based on this design. IIRC, the energetic he used was a
fairly fast one (ETN, PETN or maybe RDX). There was pictures of a test he made.
|
|
NeonPulse
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 417
Registered: 29-6-2013
Location: The other end of the internet.
Member Is Offline
Mood: Isolated from Reality! For Real this time....
|
|
https://www.sciencemadness.org/whisper/viewthread.php?tid=33... This is the thread I presume. It was a great idea.
|
|
Rocinante
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 121
Registered: 13-11-2017
Member Is Offline
Mood: No Mood
|
|
For RDX: https://www.sciencedirect.com/science/article/pii/S001021801...
https://www.researchgate.net/publication/292989139_Thermobar...
|
|
joseph6355
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 144
Registered: 23-8-2017
Member Is Offline
Mood: Nitrated
|
|
So this is basically Detcord, but with aluminum foil?
The idea seems nice at first.
The main purpose of detcord is to detonate other explosives. I don't see how a thermobaric device would help on that.
I think that Liptakov has other uses in mind besides detcord.
Oh, hello! ![:)](./images/smilies/smile.gif)
|
|
Laboratory of Liptakov
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1367
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
If someone wants to beat a tree, the biggest problem is placing the charge around the tree. From all sides. Because if the charge is from all sides,
it is most effective. Thus, less EM grams is necessary. Wrappolite is used as an adhesive tape. Use is same as bandage. Inside can be almost
anything. For example KClO3 + WD40. Full strenght from No.8 . Even 2cm diameter only. Incredible powerful........
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
I have seen the results of wrapping a tree with several wraps (recall it was 5 or 6 times around the tree) of fairly heavy det cord (40 grains/foot).
All it did was remove the bark and a small ammount of wood directly under the wrapping of cord- this was on a young oak tree about 8" thick. That
would work out to about 8 grams of PETN, if it had been drilled into center of tree and the hole stemmed, would have done more dammage.
How much would 24" of the 2cm Chlorate:WD40 aluminum foiled charge weigh?
I was taught to drill the tree mostly through, tamp the charge to expand it against the bored hole, then stem with clay, wet sand, etc.
|
|
joseph6355
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 144
Registered: 23-8-2017
Member Is Offline
Mood: Nitrated
|
|
Quote: Originally posted by Bert ![](images/xpblue/lastpost.gif) | I have seen the results of wrapping a tree with several wraps (recall it was 5 or 6 times around the tree) of fairly heavy det cord (40 grains/foot).
All it did was remove the bark and a small ammount of wood directly under the wrapping of cord- this was on a young oak tree about 8" thick. That
would work out to about 8 grams of PETN, if it had been drilled into center of tree and the hole stemmed, would have done more dammage.
How much would 24" of the 2cm Chlorate:WD40 aluminum foiled charge weigh?
I was taught to drill the tree mostly through, tamp the charge to expand it against the bored hole, then stem with clay, wet sand, etc.
|
The problem is that most of the energy delivered by the exploson is dispersed in the air, and not focused on the tree.
If you drill a hole in the middle of the stump and then pack and close it with HE, all of the energy will be used to shred it in hundreds of pieces.
Detcord on the other hand, will disperse its energy at all directions instead of focusing it in a specifc spot or area.
I don't know how the wrappolite would perform. I'm certain that a higher amount of HE would do more damage obviously, but would it be enough?
[Edited on 10/2/18 by joseph6355]
Oh, hello! ![:)](./images/smilies/smile.gif)
|
|
Laboratory of Liptakov
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1367
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
Explosion from central hole is of course much more efficiency. If we can use electric tools, drills, we can use also electric saw or next tools on
the wood. It what is on picture works. AN + EG or PCh + WD40. In stechio balance on - 20. Foil is about 10% of mass. Density low, less than 1. Can be
even 0,5g/cc. 20 cm tree is pretty enough. On it is better use central hole. Because weight of EM is neccessary counting EM2 from diameter.
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|