Proper tubing for vacuum - what works best?
I have some thick nylon (thread) reinforced vinyl tubing that works pretty well for vacuum but when it gets warm, the tube still collapses. Is this
adequate tubing and I need to figure a way to mitigate the heat issue or is there a more rigid tubing type that can withstand temps (~140F)?
|
|
Heavy Walter
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 127
Registered: 17-12-2015
Location: Argentina
Member Is Offline
Mood: No Mood
|
|
vacuum hose
Hi
There are some reinforced with a spring.
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1701
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
You could try running a length of coarse rope through the tube. At high vacuum the flow rate is usually negligible.
We're not banging rocks together here. We know how to put a man back together.
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Buy red rubber hose for vacuum at Carolina Biological.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
RogueRose
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1590
Registered: 16-6-2014
Member Is Offline
|
|
Thanks for the replies. The idea of putting a rope in the middle is attractive!..
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
I find that orange/black gas pipe is rigid enough and easily available.
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1701
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Rigid rubber hoses used for gas and petrol usually work fine. I discovered the other trick while vacuum-bagging some fiber glass, the cheap hose I had
available would collapse quite fast. Stuffing it with breather cloth was enough, a bit of rope should do the same.
We're not banging rocks together here. We know how to put a man back together.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Fulmen ![](images/xpblue/lastpost.gif) | You could try running a length of coarse rope through the tube. At high vacuum the flow rate is usually negligible. |
It certainly would be.
The flow rate is low but (obviously) the pressure available to drive that flow rate is tiny.
Vacuum systems use big wide pipes for a reason; filling them with rope will massively reduce the pumping speed.
Filling a big tube with a bunch of smaller tubes is less bad.
"wedging" the pipe open with a spring is one of the better options- that's why the commercial products do it that way.
|
|
Radium212
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 85
Registered: 26-6-2017
Member Is Offline
Mood: Pyrophoric.
|
|
I tend to use tubing only when necessary, and have many lengths of bent or straight copper pipe. I join the copper pipe to other things with small
pieces of silicon tubing, but keep it short enough that it can't really collapse.
|
|
happyfooddance
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 530
Registered: 9-11-2017
Location: Los Angeles, Ca.
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Radium212 ![](images/xpblue/lastpost.gif) | I tend to use tubing only when necessary, and have many lengths of bent or straight copper pipe. I join the copper pipe to other things with small
pieces of silicon tubing, but keep it short enough that it can't really collapse. |
I do the same thing, except I use hdpe tubing. It is pretty easy to handle, and you can shape the tubing with heat if need be.
|
|
happyfooddance
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 530
Registered: 9-11-2017
Location: Los Angeles, Ca.
Member Is Offline
Mood: No Mood
|
|
Magpie, how does this hose do with acids? Nitric, HCl, etc...? I have seen it before, it looks very nice to deal with except for being opaque.
|
|
Cezium
Harmless
Posts: 39
Registered: 5-1-2015
Member Is Offline
Mood: No Mood
|
|
Used something like this and it is good enough, doesn't collapse even with two stage oil vacuum pump and is also decently chemically resistant.
https://www.ebay.com/itm/Blue-4mm-Vacuum-Silicome-Hose-Inter...
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Quote: Originally posted by happyfooddance ![](images/xpblue/lastpost.gif) |
Magpie, how does this hose do with acids? Nitric, HCl, etc...? I have seen it before, it looks very nice to deal with except for being opaque.
|
It is very nice to deal with. I have used it in all my experiments for years with no sign of chemical attack.
If you submerged it in nitric acid overnight I suspect it would be degraded.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
DrP
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 625
Registered: 28-9-2005
Member Is Offline
Mood: exothermic
|
|
I used to use silicone rubber. I preferred it to the red tubing in case any solvents accidently got sucked into it... they come back out red! lol.
I used rubber bungs made from clear silicone rubber too as solvents don't leach out the red dye.
PS - Actually - sorry, the stoppers were silicone rubber, I do not know what the tubing was - Was clear though to avoid red dye from the rubber
getting dissolved in.
\"It\'s a man\'s obligation to stick his boneration in a women\'s separation; this sort of penetration will increase the population of the younger
generation\" - Eric Cartman
|
|
Electra
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 179
Registered: 11-12-2013
Member Is Offline
Mood: No Mood
|
|
The cheapest solution I can recommend is black rubber hose from your local automotive store. I usually get 3/8" ID rubber hose from autozone or a
similar store, and they cut it to any length you want. So far this is the cheapest and strongest vacuum hosing I have come across. I've never had
issues with it collapsing under vacuum at all. I can't even force it to collapse by pulling a full vacuum and squeezing it, it's just too thick, as it
is rated to positive pressures of 100-250psi. So far I've used this hosing for over 2 years and have never had any issues with solvents or degradation
of the hose, despite how often solvents get sucked through my vacuum.
The hoses you find on scientific supply websites are similar in thickness, but you will certainly pay much more.
https://www.autozone.com/plumbing-hosing/rubber-hose
[Edited on 14-1-2018 by Electra]
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
I finally called CarolinaBiological, it seems their website is down.
They want $44/50ft. Don't sell it by the foot. I used to be able to buy it in 15ft sections.
The price is good if you can buy 50ft.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
NEMO-Chemistry
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline
Mood: No Mood
|
|
I use same stuff they use for propane etc, the fairly rigid orange stuff. Or I use black thick airline type.
|
|