Is Samarium really this cheap?
So I always wanted to explore the chemistry of rare earth metals and I began looking for the cheapest ones on eBay and I found this user selling 100g
of 99% pure Samarium metal powder for 30 bucks...
http://www.ebay.com/itm/100g-3-52-oz-99-9-High-Purity-Samari...
I know nothing about rare earth metals yet and neither about their prices so I began wondering if this was actually real or just a fake... You would
expect rare earth metals to be quite expensive because, well... they are rare... right?
I really appreciate any help guys
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6251
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Rare Earths aren't that rare. But they are (or were) difficult to separate. They are naturally found altogether in the same ores.
Now that they are used extensively in electronics, cheaper and more efficient methods for separating have been developed. Of course the proportions
in which they are produced is not the same as the proportion in which they are used. It is likely that you are benefitting from a surplus somewhere.
|
|
PirateDocBrown
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline
Mood: No Mood
|
|
True! Neodymium, lanthanum, and yttrium are all more common than cobalt.
And the most common, cerium, is nearly as common as copper.
Even the rarest, lutetium, is about the same as thallium.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
That picture looks a lot more like samarium oxide than any metal.
|
|
BlackDragon2712
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 124
Registered: 22-12-2012
Location: Everywhere
Member Is Offline
Mood: Sleepy
|
|
Yeah and it looks the same as this one just with a different letter:
http://www.ebay.com/itm/100g-3-52-oz-99-99-High-Purity-Lanth...
mmm... I'm going to risk it and buy it... I hope there is at least rare earth metals on there. I'm going to buy the lanthanum one though, the seller
has higher ratings and is cheaper just in case it's a fake
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
That looks like it could be this stuff: https://m.youtube.com/watch?v=nOo1XMesdS0
I made that video of an attempt to purify it. Ended up with a somewhat cleaner, pale yellow "lanthanide carbonate" but it doesn't appear to be pure
lanthanum. I got the powder from Brain&Force who in turn got it from diddi. Not sure of the original source, but it looks very similar.
|
|
BlackDragon2712
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 124
Registered: 22-12-2012
Location: Everywhere
Member Is Offline
Mood: Sleepy
|
|
Yes it looks very similar indeed... and the fact that it is in a Ziploc bag and still "99.99% pure" I think is a straight up lie... I wonder how
impure it is though.
Zts16 did you find any use for the carbonate you made at the end?
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Samarium also slowly oxidizes in air to white samarium oxide. I have a bulk sample of the metal that's developed a white powdery coating over a few
years. I'd be highly skeptical that this is actually powdered metal stored in a Ziploc bag. If it is, it won't stay that way for long.
|
|