Steamboy
Harmless
Posts: 12
Registered: 24-1-2017
Member Is Offline
Mood: No Mood
|
|
Make aluminium powder of 60~30 µm
I need make aluminium powder, however, produce it using common sandpaper in aluminium foil, although effective, is slow and impractical.
Also, produced aluminium powder has a pinky-gray colour due to impurities (pink for the colorant of sandspaper), ie, aluminium can tear to common
sandpaper.
Also, I don't have coffee grinder nor other machine for create it.
What type of sandpaper can I use?
Is there better alternatives that doesn't implies the use of machines?
[Edited on 26-1-2017 by Steamboy]
|
|
Jstuyfzand
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline
Mood: Learning, Sorta.
|
|
A ball mill, closer to machineless is not going to happen.
If there is an alternative, I'd love to hear about it.
|
|
Chlorine
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 56
Registered: 26-11-2016
Location: Maine, USA
Member Is Offline
Mood: Brominated
|
|
Your best option is to buy or make a ball mill. Machined aluminum turnings work wonders because they're dirt cheap and brittle. I've tried using foil
in a ball mill and it was a disaster.
|
|
Morgan
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1675
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
Maybe by heating a roll of aluminum foil and then quenching it, it would become less ductile or embrittled enough to use.
|
|
gatosgr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 237
Registered: 7-4-2015
Member Is Offline
Mood: No Mood
|
|
You can also evaporate aluminum in vacuum and then quench it.
|
|
Meltonium
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 97
Registered: 23-9-2016
Location: Home in pajamas
Member Is Offline
Mood: Fluorinated
|
|
A nice, coarse file might work well instead of sandpaper. Although, it may be prone to clogging since aluminium is very soft.
"If at first you don't succeed, fail, fail again."
|
|