Amateurneedshelp
Harmless
Posts: 1
Registered: 7-1-2017
Member Is Offline
Mood: No Mood
|
|
Mixing liquid into resin
I'm not sure if I'm even in the right place but I've been experimenting making resin jewelry with breastmilk. Yes, I know a lot of people think it's
weird, but I cannot figure out a formula to do so without the resin either not setting right or the milk changing colors after a few weeks. Any
chemists out there have a clue on how I can preserve the breastmilk and then seal with resin? Thank you!!
|
|
D4RR3N
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 271
Registered: 9-1-2007
Member Is Offline
Mood: No Mood
|
|
Yeah your right it is weird!
You would have to dry the milk first, then add the powder to the resin
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
Soooo, wait... Whats the point of that? Not trying to be rude, but I fail to see how breast milk would enhance resin in some asthetic maner. Is
it litterally just the fact that it's breast milk?
Could you provide a picture, describe how it's changing color and why thats bad. I find nothing wierd about using different media if it provides some
maner of value to your work. You may just need some kind of antioxidant/preservative?
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
The traditional way of stabilising milks is to make cheese.
You might need to dry and powder it before mixing it into the resin.
|
|
NitratedKittens
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 131
Registered: 13-4-2015
Location: In the basket with all the other kittens
Member Is Offline
Mood: Carbonated
|
|
Maybe dry the milk then dissolve in a solvent like isopropyl alcohol or ethanol then mix with the varnish, or if that does not work try using uv
resistant resin to stop the milk from decomposing.
Also this is a chemistry forum and not really a jewellery forum.
Basket of kittens for you ........BOOM
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
The polymerisation (setting) of many resins is inhibited by air, moisture , alkalinity and acidity and many other compounds which may include alcohol.
So if your mixing milk with the resin there is a good chance it will not polymerise properly. The monomer/s tend to be reactive and may will react
with the milk to discolour it.
One option is to create a previously polymerised resin item with a cavity which is then filled with milk which is then stoppered with resin or inert
plug It can then be sealed with resin.
There are many compounds that could be used to stop the milk fermenting. Haxamine (solid fuel camping stove tablets) for example but I don’t know if
that would discolour the milk or curdle it. If the resin is unaffected perhaps sterilising the item, after its construction, in pressure cooker would
work
[Edited on 8-1-2017 by wg48]
[Edited on 8-1-2017 by wg48]
|
|
gatosgr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 237
Registered: 7-4-2015
Member Is Offline
Mood: No Mood
|
|
Regular aspirin can also be used as a preservative.
|
|