Author: Subject: Acid and Base slags in non-aqueous environment ?
metalresearcher
National Hazard
****




Posts: 790
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 3-9-2016 at 09:29
Acid and Base slags in non-aqueous environment ?


I sometimes read about acid slags (containing much SiO2) and basic slags on top of metal melts in metallurgical processes.

But are the terms 'acid' and 'base' not only for aqueous solutions as 'acid' contains H3O+ / H+ and 'base' OH- ?
And these ions are not present at all in metal slags.

What am I thinking wrong ?
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 3-9-2016 at 11:25


Quote: Originally posted by metalresearcher  
I sometimes read about acid slags (containing much SiO2) and basic slags on top of metal melts in metallurgical processes.

But are the terms 'acid' and 'base' not only for aqueous solutions as 'acid' contains H3O+ / H+ and 'base' OH- ?
And these ions are not present at all in metal slags.

What am I thinking wrong ?


The term acid and base in this context goes back a couple of centuries.

Oxides were once categorised as 'acid formers' or 'base formers' (to some extent that is still true but acid/base theory has evolved enormously since then).

'Acid forming oxides' (in slags) are mainly Silica which (in theory) forms silicic acid (simplest form H2SiO3) which forms silicates. Slag silica can be 'neutralised' by strong bases like lime (or limestone).

'Base forming oxides' by contrast would be CaO, Na2O, K2O, alumina (an amphoteric oxide) etc.

Silica is mostly the result of residual gangue material accompanying the target ore (e.g. iron ore).

[Edited on 3-9-2016 by blogfast25]




View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4412
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 3-9-2016 at 12:03


There are several definitions of acids and bases, the most common being the Bronsted-Lowry definition (acids give up H+, bases accept H+). There's also the not-maligned-enough Arrhenius definition (acids contain H+, bases contain OH-, so that ammonia and carbonate aren't really bases, but "base analogues", so nobody ever uses that one except in high school textbooks), the Lux-Flood definition (acids accept oxide ions, bases contribute oxide ion, which is useful for slags and melts), and the Lewis definition (an acid accepts an electron pair, and a base contribute an electron pair).

So a reaction like Na2O + SiO2 -> Na2SiO3 is an acid-base reaction according to the Lewis and Lux-Flood definitions. Same with CaO + SO3 -> CaSO4




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.