Hello,
recently I´ve prepared 50 grams of pure silver nitrate. They are packed in two plastic bottles - 25 g each. It was prepared by dissolving relatively
pure silver metal (97-98%) in high grade concentrated nitric acid. The product was recrystallized two times from distilled water. The first fraction
of crystallization is really pure (99%+). The second is a mix of the first fraction and the second one, but still appreciable quality. U2U if
interested. ![:)](./images/smilies/smile.gif)
1 x 25 g for 20$/25g + shipping (ca. 5$ - depends on locality) - 99%+
<img src="http://chem.pieceofscience.com/wp-content/uploads/2016/05/SN4.jpg" style="width:600px;height:600px;">
Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
That batch you sold me is Great.
Better than my own prep, judged only by the colour.
You're obsessed with the stuff.
When you've sold it all, move on to Uranium Nitrate
|
|
DutchChemistryBox
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 74
Registered: 24-3-2013
Location: Strasbourg
Member Is Offline
Mood: No Mood
|
|
"The first fraction of crystallization is really pure (99%+)."
What is your method of assay?
|
|
Hegi
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 199
Registered: 27-9-2013
Member Is Offline
Mood: No idea.
|
|
That is really good question. I haven´t done an analysis of the product but assuming the silver was pure enough, HNO3 as well. The product was
recrystallized two times from distilled water, filtered off (leaving approximately another 40 grams of the substance in the solution with impurities
of course), washed with little amount of ice cold distilled water dried in the dark for 5 days.