My single-stage, single-vane vac pump failed to pump today, so i pulled it apart.
Here's the Innards with just the oil resevoir removed:
This is some goop that was in there (it started as a clear oil) :
![goop.JPG - 203kB](http://www.sciencemadness.org/talk/files.php?pid=447117&aid=50281)
It feels lumpy and a bit rubbery, similar to broken up bits of the factice i made some time ago.
Hardly surprising seeing as no end of nasty liquids and gasses have gone into it.
Disassembly is dirty and oily, as will be the cleanup and fixing.
Lesson learned : always use a crap-trap in line with the vac pump or it will get broken.
The real shame is that i had already integrated it into my new fume hood.
The shiny new (and illuminated!) button got pressed for Vacuum and just a distressed buzzing sound happened, no vacuum ![:(](./images/smilies/sad.gif)
Thinking of vinegar or dilute phosphoric acid to rip all the rust out.
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Vacuum pump abuse is one of society's most heinous crimes.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
I was thinking of posting in 'The Cops Showed Up' thread, but they didn't.
Vac pump abuse like this goes on behind closed doors all the time.
If any pumps are affected by this post, please visit www.pumpline.com for help and advice.
|
|
Loptr
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
I freaked out a while back when hose full of solvent made a straight-shot from the vacuum-take off adapter (not sure exactly how it happened) and into
the pump. I pulled the pump apart shortly afterwards to clean the innards and the pump ended up being alright after that. The damage that it did incur
was to a filter can that sits in between the hose barbs and the pump itself--a corrosion took place that caused it to grow a beard on the bottom of
the can. It looked like a little gnome without a body, and a little similar the nitric acid gnomes I saw back at school.
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
LOL.
Brilliant description Loptr, just brilliant.
|
|
Detonationology
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
I was running a nitric vacuum distillation today, using the double trap method. I had my pump open a few weeks ago for cleaning, but for some reason,
all 4 of the vanes were seized when I went to start it up-- not a single mm of Hg. Not happy when I took it apart to realize that some black goop
plastered the vanes into place. A washed with acetone and wiped with a rag, then used the air compressor to blow out any dry crud. Not sure if it
was caused by my choice of oil or simple from neglect.
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
The choice of oil seems quite important.
Currently all i have that appears suitable is 'baby oil' (some slightly watered mineral oil).
I;ve heated it before and it gives off vapours and goes a bit brown : i expect that it's better boiled for a while before sticking in a vac pump.
|
|
Chemist_Cup_Noodles
Harmless
Posts: 46
Registered: 27-5-2015
Location: Northern VA
Member Is Offline
Mood: Anticipative
|
|
Hm, what about a silicon based oil? Similar to one that you might use for a lab oil bath and also a lubricant? They seem kind of pricy, but idk if
they would work or not. Surely they are quite inert though, so it shouldn't f*ck up your pump like baby oil did. But tbh it looks like you skipped the
oil part of baby oil and flung baby shit all in there.
I'll be honest-- We're throwing science at the wall here to see what sticks. No idea what it'll do.
-Cave Johnson, Portal 2
Add yourself to this map of SciMad members! https://zeemaps.com/map?group=388676&add=1
|
|
NedsHead
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 409
Registered: 9-12-2014
Location: South Australia
Member Is Offline
Mood: No Mood
|
|
When the local heating/cooling supply store is out of vacuum pump oil I use pneumatic tool oil, it works just fine
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
This is also one of the most under-reported crimes because of the stigma. Thank you for having the courage to report this.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Hey. I don't feel so bad now.
I inadvertently did violence to my diaphragm pump a few months ago.
I put some iodine vapours through it which I don't think helped the aluminium parts very much. I also flooded it by not looking how full my filter
flask was getting. And, like an idiot, I did not disassemble and clean it right away. I did not appreciate the damage until the next day when I
turned it on and there was no suck at all.
But the gaskets were still intact. It responded well to the cleaning out of crap. The inside does not look so pretty but it is still functional. And
I have made a solemn promise with a boy scout salute to never suck nasties without a trap.
You could probably call me a reformed pump abuser. But the truth is that I still have not constructed or purchased a decent trap.
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1638
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by NedsHead ![](images/xpblue/lastpost.gif) | When the local heating/cooling supply store is out of vacuum pump oil I use pneumatic tool oil, it works just fine |
Won't for too long though.
Hydroshocked Dry Mineral oil or a synthetic Silicon rated for vacuum pumps. Synthetic silicon ones are the best IMO.
Very good scrubber then mechanical filter, better would be Wet scrubber> Drying scrubber > Mechanical 1uM filter.
Trick is preheat the pump (Let run blanked off till at operating temp)
This will maximize the health and life of your pump, in refrigeration we can't do as all of that but I all ways use a large filter dryer on mine to
help protect from contaminants
To flush a pump out drain off half the oil, measure out a fresh bit of oil matching the drained portion, slowly feed it into the intake so it flows
through the vans, drain all oil from pump, pulse on for a second and no longer, refill with fresh oil, and run till at operating temp, continue for 10
minutes then shut down and release the vacuum.
Filters and oil are much cheaper then a new pump! and to make a solid scrubber filter system is very easy! 2 - 1L Erlenmeyer flasks and a water
cartridge filter would do the job impeccably.
1l wet scrubber, 1L drying scrubber then the 1micron water filter to remove any particles that made it through
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Currently this poor pump is undergoing emergency surgery.
Amazing how well phosphoric acid rips the rust off, especially with a toothpick to scratch off the sludge.
Most of the bits are now rust-free under mineral oil, awaiting re-assembly.
Doing the big casting part at the mo.
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1638
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
inspect the bore care fully the finest of scratches will obliterate its vac capability
[Edited on 29-4-2016 by XeonTheMGPony]
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
I did wonder about stuff like that, hence using a wooden toothpick rather than a metal scraper (e.g. screwdriver).
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Wow ! I'm impressed !
Here's how it looks after a few hours in ~50% phosphoric acid with some gentle scraping.
![casting.JPG - 200kB](http://www.sciencemadness.org/talk/files.php?pid=447278&aid=50291)
The shine is due to some mineral oil coating to keep the air out.
[Edited on 29-4-2016 by aga]
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1638
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
If the bore has been gouged or has pits in it and they are not too deep you can recover it by care full honing with a brake cylinder hone with a
constant slow flow of mineral oil in a cross thatch pattern, but you'll probably need to get new blades.
Once that is don run for 30 minutes with fresh mineral oil, power purge (Dribble oil into the intake port while running) then drain refill with fresh
oil and let run for an hour. Both runs are don with a tiny bit of air allowed to run through.
After this it should pull a good vacuum again, not like new, but use full.
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
The 'bore' by which i assume you mean the hole that the vanes spin in, that part is clean and scratch-free.
We'll see if it works when the cleanup/reassembly is done, so try not to lose too much sleep.
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1638
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
that's a good thing then!
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Puzzle Pump
Well, these are all the actual pump Bits.
![Bits.JPG - 145kB](http://www.sciencemadness.org/talk/files.php?pid=447336&aid=50318)
They all came Out, so i guess they all go back In somehow ...
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Success !
![Done.JPG - 128kB](http://www.sciencemadness.org/talk/files.php?pid=447340&aid=50322)
Thanks to the support of all the VPAA people out there.
(vac pump abusers anonymous)
Edit:
Rigged up to the 'hood it reads at about 20 mbar (15 torr) which i think is roughly what it has always shown as it's best vacuum.
[Edited on 30-4-2016 by aga]
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2690
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
Just changing the oil occasionally will do wonders, but I will admit that we often only change it every 6-12 months, but we do have a trap or two for
most pumps, and try to keep them cold with dry ice at all times. But the Welch I mostly use (at work) has been in use for 5 years without any
issues, and it was old when I got it. The other one I use now, another old Welch, looks even older, if too small for the number of things on it, and
barely restarts if turned off, but still pulls a decent vacuum. But I know it is on borrowed time, it looks older than I do, and sounds worse. We
did just change the oil, but the sight glass is so old and filthy, that it is barely even possible to see the fill line, have to use a strong
flashlight.
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Today i got some 'proper' vac pump oil, so changed out the Baby Oil that i'd used as a stop-gap.
With the Baby oil i got 20 mbar.
With 'Proper' oil i get 100 !!!
Edit:
That's 80 mbar WORSE in case anyone was wondering.
[Edited on 5-5-2016 by aga]
|
|
Loptr
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
Quote: Originally posted by aga ![](images/xpblue/lastpost.gif) | Success !
Thanks to the support of all the VPAA people out there.
(vac pump abusers anonymous)
Edit:
Rigged up to the 'hood it reads at about 20 mbar (15 torr) which i think is roughly what it has always shown as it's best vacuum.
[Edited on 30-4-2016 by aga] |
aga, got an extra room? I think I might come to stay with you for a while. The background in your photo is gorgeous!
My backyard is a graveyard and a university. Kind of strange.
[Edited on 5-5-2016 by Loptr]
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
There is one extra room, although that's reserved for the kids if/when they want to come home for a while.
Basically No, and you can't come and live in my new fume hood either.
Yeah, i do kind of live in paradise.
'Paradise' all depends on your state of mind.
Most places are Paradise, just takes the Eyes to See.
If you do not like where you live then you can Move to somewhere Different.
I did 10 years ago, and do not regret it at all, quite the opposite.
|
|
Pages:
1
2 |