What to use for grinding alumina?
I have some alumina boats that I bought for my tube furnace, and they are a fraction of a millimeter too big to fit into my quartz tube. I'd like to
grind them down so they will fit and have a little room to expand, and I'm not sure what could grind alumina other than a diamond grinding wheel. Is
that my only option, or are there other grinding wheels that can grind alumina?
|
|
NedsHead
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 409
Registered: 9-12-2014
Location: South Australia
Member Is Offline
Mood: No Mood
|
|
Silicon carbide (green wheel) should be able to do it, I use one to grind tungsten carbide lathe tools, it's harder than an aluminium oxide wheel but
softer than diamond, I would guess it can cut through alumina
|
|
JJay
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3440
Registered: 15-10-2015
Member Is Offline
|
|
I wonder if I have any silicon carbide dremel wheels around here anywhere....
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3625
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
I just did a quick calculation;
for 1000C temperature rise the difference in linear thermal expansion between quartz and alumina is 0.7%
i.e. for a 50mm int. dia tube an extra 0.35 mm grinding compared to a sliding fit ![:P](./images/smilies/tongue.gif)
I think that principle is correct, the calculations may not be, check.
|
|