Fluorinert FC-40
I was recently (extremely) lucky enough to become the recipient of a large quantity of a very interesting substance, Fluorinert FC-40: http://solutions.3m.com/wps/portal/3M/en_US/Electronics_NA/E...
Fun Facts:
- An electrically insulating liquid used mainly for cooling electronics (by convection).
- True to it's name, it's very chemically inert.
- It is capable of dissolving large amounts of gases. Because of this, it was used in the movie The Abyss as the underwater oxygenated breathing
liquid. It was actually breathed by a rat in the movie, but the actors used special effects instead (since the rats tended to die a few days after
breathing it).
- It's viscosity is about the same as water and it's colorless, but it is almost twice as dense as water. Hefting the little jugs I have is very
surprising.
- BP range of 150 - 175 degrees C
I now have several liters of this liquid, and would love to find some interesting uses for it. Applied Science made an interesting video where he used
it to fry a potato chip. My first hope was to use it as a dense solvent for the potassium synthesis (see the stickied thread), but the boiling point
appears to be too low. Any ideas for fun projects that require an inert, dense, nonpolar solvent?
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by MrHomeScientist | My first hope was to use it as a dense solvent for the potassium synthesis (see the stickied thread), but the boiling point appears to be too low. Any
ideas for fun projects that require an inert, dense, nonpolar solvent? |
That would be a bad idea. K is capable or ripping F from these molecules and quite exothermically too!
Similar stuff has been used as mild fluorinating agents, e.g. conversion of metal oxides to metal fluorides, at fairly high temperature.
Generic example:
6 MeO + C6F14 === > 6 MeF2 + 6 CO2
Beats using F2 or chlorine fluorides, in terms of safety!
Think e.g.
7 Nd2O3 + 3 C6F14 === > 14 NdF3 + 3 CO2 + 15 CO
[Edited on 6-1-2016 by blogfast25]
|
|
Bert
Super Administrator
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
I could see some exciting reactions with finely powdered. Mg, Al or alloys...
Mechanical uses for buffers/inertial dampers?
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Considering just how vigorous both these metals react with PTFE (Teflon) and that we're dealing with a fairly low boiler, those reactions might be
difficult to contain.
|
|
MrHomeScientist
International Hazard
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by blogfast25 | Similar stuff has been used as mild fluorinating agents, e.g. conversion of metal oxides to metal fluorides, at fairly high temperature.
...
7 Nd2O3 + 3 C6F14 === > 14 NdF3 + 3 CO2 + 15 CO
|
Since this is a fairly low boiling solvent, how would such a fairly high temperature reaction be done practically? High pressure, sealed container?
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by MrHomeScientist |
Since this is a fairly low boiling solvent, how would such a fairly high temperature reaction be done practically? High pressure, sealed container?
|
A tubular reactor contains the target oxide and is heated to a suitable temperature.
A boiler containing the FC-40 is attached to it and heated till it starts boiling. These vapours are thus lead over the heated oxide. Control vapour
delivery by heat input to the boiler.
Post-reaction, a simple condenser separates any unreacted FC-40 from the carbon oxides.
There's a fluoridation reaction of UO2 to UF4 ('green salt') with a Classic CFC in the library's Brauer ('Handbook of Inorganic
Preparations').
An interesting one could be CuO to CuF2, as one is black and the other green. And CuO isn't the stablest of oxides (in terms of EoF), so
success is 'guaranteed'.
[Edited on 6-1-2016 by blogfast25]
|
|
unionised
International Hazard
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Just a quick thought, look out for COF2 and HF as potential by-products.
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
HF? There's probably no H in the FC-40...
|
|
MrHomeScientist
International Hazard
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Indeed, it's claimed to be fully fluorinated. Nothing but C's and F's. But potassium could rip it apart? I was under the impression that fluorine
bonds were very hard to break.
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by MrHomeScientist | Indeed, it's claimed to be fully fluorinated. Nothing but C's and F's. But potassium could rip it apart? I was under the impression that fluorine
bonds were very hard to break. |
They are but:
(CF2)n + 2 n K === > 2 n KF + n C
... is still exothermic @ STP by about - 50 kJ/mol of K.
Teflon stirrers bars have been shown to be blackened in the KOH/Mg reduction.
[Edited on 6-1-2016 by blogfast25]
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Other applications could be as a highly inert, aprotic, non-polar solvent in some organic reactions. The BP would allow for some really hot refluxing.
But no specific examples really jump to my mind...
|
|