nicamarvin
Harmless
Posts: 3
Registered: 30-10-2015
Member Is Offline
Mood: No Mood
|
|
Spray On Copper Mirrors
good afternoon good people, My Name is Marvin from Nicaragua, I am not new to the Brashear process of making silver mirrors, I currently Spray Silver
Mirrors and Plastics(Spray On Chrome) How hard do you think would be using Copper instead of Silver in the process?(changing Silver Nitrate for Copper
Nitrate all else remaining the same)
|
|
Detonationology
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
I don't have any practical experience with making mirrors, but I don't see why it wouldn't work. However, I doubt it would be very reflective at all
by itself. Maybe you could do a mix with silver and copper to have better results.
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
WGTR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline
Mood: Outline
|
|
You will probably have more success depositing copper onto a silver mirror, rather than depositing copper by itself.
The following patent describes a bit about this.
Attachment: US2801935.pdf (336kB) This file has been downloaded 450 times
A very useful source, if you can find it, would be Bruno Schweig's book Mirrors: A guide to the manufacture of mirrors and reflecting
surfaces.
|
|
nicamarvin
Harmless
Posts: 3
Registered: 30-10-2015
Member Is Offline
Mood: No Mood
|
|
Thanks for your replies guys, I wanted to know what were your thoughts on the matter.. I have been able to apply a Copper Mirror on surfaces(Spray On
Copper) for both Mirrors and other nonconductive surfaces like plastics, Ceramics,
check this video
https://www.youtube.com/watch?v=WnZ9hgEfw88
|
|
WGTR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline
Mood: Outline
|
|
Neat video. So, what are you using? I've sprayed on silver using a two part combination of hydrazine sulfate/ammonia, and silver nitrate/ammonia.
The surface was sensitized using a separate solution of stannous chloride.
According to Schweig, it's possible to deposit copper without silver, as long as some palladium or platinum salts are added to one part of the
mirroring solution. He noted better adhesion with a silver base coat, however.
Are you getting good adhesion, without blistering?
[Edited on 10-31-2015 by WGTR]
|
|
nicamarvin
Harmless
Posts: 3
Registered: 30-10-2015
Member Is Offline
Mood: No Mood
|
|
Copper Nitrate, Sodium Hydroxide, Amonium Hydroxide Reduced by Hydrazine,
the surface is activated by Stanous chloride first and then Palladium Chloride) I have good adhesion but that was just to let people see its possible,
for production purposes(where reducing costs are a must) I use Stanoush chloride and a Flash coat of Silver(about half way of a normal coat) adhesion
is also very good..! Palladium is Rather expensive
[Edited on 1-11-2015 by nicamarvin]
|
|