K metal from KOH, Mg, and Diacetone Alcohol
I've been studying this Nurdrage video here: https://www.youtube.com/watch?v=JAo2F9ymKXA
Nurdrage uses tertiary alcohols to catalyze KOH reduction with Mg. He does it at 200C though and tert-butanol boils at 83C. Diacetone alcohol is
also a tertiary alcohol but boils at 160C. It'd be nice to do the reaction without reflux. Has anyone ever tried this? I wonder if the ketone group
would interfere with the reaction? I'm contemplating trying it out but curious to see if anyone else has tried it.
[Edited on 11-10-2015 by runninfarmer]
[Edited on 11-10-2015 by runninfarmer]
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6255
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
There is extensive discussion on this topic here.
http://www.sciencemadness.org/talk/viewthread.php?tid=14970
I am not sure if anyone has tried using diacetone alcohol. I don't recall reading it. You could always give it a try.
The tricky thing for most people seems to be coming up with a suitable medium to perform the reaction in. Paraffin oils are a bit hit and miss. The
oil needs to meet specific requirements and not all of them do. For this reason, I suggest duplicating the method using standard reagents and then,
having achieved success, attempting with the diacetone alcohol.
I recommend also requesting a mod to merge this with the main thread so all information is in one place.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by runninfarmer ![](images/xpblue/lastpost.gif) | I've been studying this Nurdrage video here: https://www.youtube.com/watch?v=JAo2F9ymKXA
Nurdrage uses tertiary alcohols to catalyze KOH reduction with Mg. He does it at 200C though and tert-butanol boils at 83C. Diacetone alcohol is
also a tertiary alcohol but boils at 160C. It'd be nice to do the reaction without reflux. Has anyone ever tried this? I wonder if the ketone group
would interfere with the reaction? I'm contemplating trying it out but curious to see if anyone else has tried it.
|
This really belongs in the relevant sticky thread. I suggest a moderator move it there:
http://www.sciencemadness.org/talk/viewthread.php?tid=14970&...
Per se not a bad idea but I think the oxygen from the caboxyl group will react with any K formed, assuming even it does form. Try a test tube
experiment?
[Edited on 11-10-2015 by blogfast25]
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | Paraffin oils are a bit hit and miss. The oil needs to meet specific requirements and not all of them do. For this reason, [...]
|
I have to disagree a bit here: quite a broad variety of inert/aprotic sovents were found to work: Shellsol D (Pok, Nurd, me), paraffinic oil (Nurd),
baby oil (Nurd), kerosene (me), Decalin (Nurd)... all worked.
As long as it's dry, BP around C and aprotic/inert it will work in all likelihood.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6255
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Quote: Originally posted by blogfast25 ![](images/xpblue/lastpost.gif) | Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | Paraffin oils are a bit hit and miss. The oil needs to meet specific requirements and not all of them do. For this reason, [...]
|
I have to disagree a bit here: quite a broad variety of inert/aprotic sovents were found to work: Shellsol D (Pok, Nurd, me), paraffinic oil (Nurd),
baby oil (Nurd), kerosene (me), Decalin (Nurd)... all worked.
As long as it's dry, BP around C and aprotic/inert it will work in all likelihood. |
Ok. Paraphrase. Mine didn't work. I am looking for an alternative oil. Kero was next on my list.
|
|