making nano particle solution with polyphenols
In the experiment in this video the guy makes suspended Iron nano particles simply by mixing polyphenols from green tea with a dissolved solution of
an Iron salt.
I wanted to know what other metal salts would this method work with and also could I use this method to make boron nano particles by mixing borax or
boric acid with green tea.
https://www.youtube.com/watch?v=rDcZleqvGKA
|
|
battoussai114
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 235
Registered: 18-2-2015
Member Is Offline
Mood: Not bad.... Not bad.
|
|
Right now I don't have the article in my hands, but I've read about reduction of copper and some other more noble metals using tea.
Batoussai.
|
|
D4RR3N
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 271
Registered: 9-1-2007
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by battoussai114 ![](images/xpblue/lastpost.gif) | Right now I don't have the article in my hands, but I've read about reduction of copper and some other more noble metals using tea.
|
Yes I have read it works for gold, they were using this method to produce gold nano particles to target cancer cells.
|
|
D4RR3N
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 271
Registered: 9-1-2007
Member Is Offline
Mood: No Mood
|
|
As I had some borax and green tea kicking about I mixed a solution of both together and observed no color change unlike the reaction in the vid. Not
sure if we would expect a color change in all instances.
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
The Metals are complexing with the polyphenols in the Tea, and there are some rules that determine what works and what doesn't.
Borax isn't like iron (iii) chloride because the Iron is in the +3 oxidation state and in sodium tetraborate the Boron is in the ...
Oh dear. All fell to bits already. Feck.
Can some proper chemist please explain what not-happens with borax and green tea, please.
|
|
Dan Vizine
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 628
Registered: 4-4-2014
Location: Tonawanda, New York
Member Is Offline
Mood: High Resistance
|
|
You simply don't have a reductant in tea with a sufficiently high reducing potential to touch borax. The metal salt examples of things that will
produce reduced products all have modest positive reduction potentials. Just look all a table of standard electrode potentials.
If you had produced boron, it would be grey-black (and also impossible, since you can't do it in an aqueous solution because the hydrogen in the water
would be reduced first).
[Edited on 21-9-2015 by Dan Vizine]