Author: Subject: Rust stain remover H3PO4
madscientist
National Hazard
****




Posts: 962
Registered: 19-5-2002
Location: American Midwest
Member Is Offline

Mood: pyrophoric

[*] posted on 6-8-2002 at 11:10
Rust stain remover H3PO4


Does anyone know the concentration of the "rust stain remover" type H3PO4 that is found at hardware stores?



I weep at the sight of flaming acetic anhydride.
View user's profile View All Posts By User
madscientist
National Hazard
****




Posts: 962
Registered: 19-5-2002
Location: American Midwest
Member Is Offline

Mood: pyrophoric

[*] posted on 6-8-2002 at 21:40


My H3PO4 is a thick, syrupy liquid. According to my references, H3PO4 that is a thick, syrupy liquid is at about 85% concentration.



I weep at the sight of flaming acetic anhydride.
View user's profile View All Posts By User
vulture
Forum Gatekeeper
*****




Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 20-8-2002 at 08:56


The maximum I've seen is 30%.
85% H3PO4 is extremely hygroscopic, see if it will dry NH4NO3.

Since I have 2L of the 85% stuff I might very well build a dessicator one day.




One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
View user's profile View All Posts By User
Ramiel
Vicious like a ferret
***




Posts: 484
Registered: 19-8-2002
Location: Room at the Back, Australia
Member Is Offline

Mood: Semi-demented

[*] posted on 5-9-2002 at 01:02
Just a thought...


I know concentrated Phosphoric acid of a known molarity can be obtained from food suppliers.
View user's profile View All Posts By User This user has MSN Messenger
a_bab
Hazard to Others
***




Posts: 458
Registered: 15-9-2002
Member Is Offline

Mood: Angry !!!!!111111...2?!

[*] posted on 16-9-2002 at 06:32


Yeah, it is used in our daily coke as acidifiant; the trucks used to transport concentrated coke syrup are labeled as "corrosive" ! And a nail will be VERY coroded if kept for 3 days in coke.
View user's profile View All Posts By User
Ramiel
Vicious like a ferret
***




Posts: 484
Registered: 19-8-2002
Location: Room at the Back, Australia
Member Is Offline

Mood: Semi-demented

[*] posted on 17-9-2002 at 00:52


I heard that it dissolves a T-Bone steak overnight.... although that's what the dentists tell you.
View user's profile View All Posts By User This user has MSN Messenger
E Beer
Harmless
*




Posts: 1
Registered: 14-9-2015
Member Is Offline

Mood: No Mood

[*] posted on 14-9-2015 at 21:42


How do you turn phosphorus acid crystals into a liquid similar to 50% hypo phosphorous acid?
View user's profile View All Posts By User
ave369
Eastern European Lady of Mad Science
****




Posts: 596
Registered: 8-7-2015
Location: No Location
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2015 at 10:13


I dunno what hypophosphorous acid looks like, never seen a specimen. But to turn solid phosphoric acid into a liquid, just add water.



Smells like ammonia....