Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
Gelling agents
Somebody has experience on gelling agents?
I want to make liquid paraffin Gel
I dont know what gelling agents are suitable for hydrocarbons
|
|
Bot0nist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline
Mood: Streching my cotyledons.
|
|
Would any of the gelling agents used for making "napalms" from gasoline not be suitable for use with such a hydrocarbon?
U.T.F.S.E. and learn the joys of autodidacticism!
Don't judge each day only by the harvest you reap, but also by the seeds you sow.
|
|
gatosgr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 237
Registered: 7-4-2015
Member Is Offline
Mood: No Mood
|
|
isnt that petroleum jelly?
from what I found out you can use aluminum stearate
[Edited on 8-6-2015 by gatosgr]
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
Thanks ,
I want to make transparent gel hydrocarbon
Does Aluminium Stearate or another Aluminium fatty acid make hydrocarbon transparent gel?
|
|
gatosgr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 237
Registered: 7-4-2015
Member Is Offline
Mood: No Mood
|
|
I dont know but to make aluminum stearate you can react steric acid with NaOH to make sodium stearate and then react it with AlCl3
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1704
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Dissolving clear polystyrene (CD-covers for instance) in gasolin works well. A bit of xylene seems to improve gelling.
We're not banging rocks together here. We know how to put a man back together.
|
|
smaerd
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1262
Registered: 23-1-2010
Member Is Offline
Mood: hmm...
|
|
I'm not sure if this is helpful at all but the paint stripper that people distil dichloromethane from has a pretty wicked gel in it.
|
|
gatosgr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 237
Registered: 7-4-2015
Member Is Offline
Mood: No Mood
|
|
The polystyrene polymer swells in gasolin doesnt it? Is this how most gels are formed?
Here more about stearates:
http://cool.conservation-us.org/waac/wn/wn23/wn23-3/wn23-304...
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
Thanks guys,
Dissolving Polystyrene in gasolin wont make glue?
|
|
Bot0nist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline
Mood: Streching my cotyledons.
|
|
Not sure what you mean by glue, but adding polystyrene to gasoline makes a blob of transparent gel that turns into a translucent, cloudy white film
when dried. It may be possible to use it as a glue, but I am not sure about its strength as an adhesive.
U.T.F.S.E. and learn the joys of autodidacticism!
Don't judge each day only by the harvest you reap, but also by the seeds you sow.
|
|
agent_entropy
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 91
Registered: 17-7-2006
Location: U.S.
Member Is Offline
Mood: No Mood
|
|
Oddly, I find that some slightly more polar solvents tend to make a more homogeneous solution when dissolving polystyrene. Tetrahydrofuran, or
nitrobenzene will produce a perfectly transparent homogeneous solution. Such solutions (viscous) can absolutely be used as adhesive, especially
between pieces of bulk (non-foamed) polystyrene, as it creates a very effective solvent weld.
On the other hand gasoline, or kerosene (and strangely, acetone) will produce a blob of swollen polystyrene sitting in the solvent.
IIRC toluene and xylene also produce a homogeneous, transparent solution but I don't have any handy to test it out.
Also, what exactly do you mean by "gel"? Do you simply mean a viscous solution? Or do you mean the classical definition of gel? (ie. A substantially
dilute (mostly solvent) cross-linked system which exhibits no flow in the steady state. Such cross-links need not be chemical in nature, as there are
any number of supramolecular or physically crosslinked gels.)
[Edited on 9-6-2015 by agent_entropy]
|
|
Zombie
Forum Hillbilly
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1700
Registered: 13-1-2015
Location: Florida PanHandle
Member Is Offline
Mood: I just don't know...
|
|
Just buy a can of polyester resin for 20 bucks. It will mix with wax.
They tried to have me "put to sleep" so I came back to return the favor.
Zom.
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
I want to make gel candle.
It usually made of paraffin and polymer and i am looking for this type of polymer
[Edited on 10-6-2015 by Waffles SS]
|
|
Zombie
Forum Hillbilly
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1700
Registered: 13-1-2015
Location: Florida PanHandle
Member Is Offline
Mood: I just don't know...
|
|
Different color horse.
You should look it up then because there is NO WAX involved. It's a mineral oil base, and co-polymers blended in to stabilize the oil.
A polyester, and wax candle smells like dog turds anyway.
They tried to have me "put to sleep" so I came back to return the favor.
Zom.
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
Right now i have a solid powder that make gel Paraffin from liquid Paraffin
I use it for gel candle
I want to know what is this?
thermoplastic powder cp9000?Ethylene Copolymer?..
[Edited on 10-6-2015 by Waffles SS]
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
What is the product name?
Did you check the msds?
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
If i had known it name and MSDS then i wouldnt have created this topic
[Edited on 10-6-2015 by Waffles SS]
|
|
Mesa
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 264
Registered: 2-7-2013
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Waffles SS ![](images/xpblue/lastpost.gif) | Right now i have a solid powder that make gel Paraffin from liquid Paraffin
I use it for gel candle
I want to know what is this?
thermoplastic powder cp9000?Ethylene Copolymer?..
[Edited on 10-6-2015 by Waffles SS] |
Type your question into google.
It's the 4th link down.
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
You are making puzzle ? What question? you think i didnt search it on google?
|
|
gatosgr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 237
Registered: 7-4-2015
Member Is Offline
Mood: No Mood
|
|
If you're making them for your own use:
https://www.google.com/search?tbm=pts&hl=el&q=parraf...
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Does the powder you have now have a label?
|
|
Amnesiac
Harmless
Posts: 1
Registered: 4-12-2015
Member Is Offline
Mood: No Mood
|
|
Kraton G1650 I've used n the Past and works very well to Gell mineral oil.
http://www.kraton.com/products/kraton_g_sebs_seps.php
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
Yes,
I found out kraton 1650 is answer and i am using it
|
|
gatosgr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 237
Registered: 7-4-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by smaerd ![](images/xpblue/lastpost.gif) | I'm not sure if this is helpful at all but the paint stripper that people distil dichloromethane from has a pretty wicked gel in it.
|
From wikipedia:
Thickeners are used for thixotropic formulas to help the mixture form gel that adheres to vertical surfaces and to reduce the evaporation of the
solvents, thus prolonging the time the solvent can penetrate the paint. Cellulose-based agents, e.g., hydroxypropyl cellulose, are commonly used for
mixtures that are not extremely acidic or basic; under such conditions cellulose undergoes hydrolysis and loses effectiveness, so fumed silica is used
for these instead. Another possibility is using waxes (usually paraffin wax or polyethylene or polypropylene derivatives), or polyacrylate gels.
[Edited on 25-1-2018 by gatosgr]
|
|