Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
 Pages:  1  ..  17    19    21  ..  24
Author: Subject: The trouble with neodymium...
DalisAndy
Hazard to Others
***




Posts: 129
Registered: 8-5-2015
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2015 at 12:38


Could one use permagnetic acid, and/or carbonatic acid? And why would Oxalic acid easier? I'm just curious



Elements Collected: 19/81 (Excluding all radioactive, using placecard for those)

Any tips or good sources are welcome.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2015 at 13:02


Quote: Originally posted by DalisAndy  
Could one use permagnetic acid, and/or carbonatic acid? And why would Oxalic acid easier? I'm just curious


'permagnetic acid'? That's either an Error 101 or a Googlewhack. :D

You mean permanganetic acid. "HMnO<sub>4</sub>". Doesn't REALLY exist. Potassium permanganate + sulphuric acid would work but NO ONE would do it like that.

You mean carbonic acid. That's soda water, basically. Do YOU think that would work? (Hint: NO!)

The oxalates of Nd and Fe are basically insoluble. It's a recipe for stalled reaction/big mess.

Go down the hardware store and get some 'muriatic acid' (HCl) or toilet drainer (H2SO4).




View user's profile View All Posts By User
DalisAndy
Hazard to Others
***




Posts: 129
Registered: 8-5-2015
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2015 at 13:36


Quote: Originally posted by blogfast25  
Quote: Originally posted by DalisAndy  
Could one use permagnetic acid, and/or carbonatic acid? And why would Oxalic acid easier? I'm just curious


'permagnetic acid'? That's either an Error 101 or a Googlewhack. :D

You mean permanganetic acid. "HMnO<sub>4</sub>". Doesn't REALLY exist. Potassium permanganate + sulphuric acid would work but NO ONE would do it like that.

You mean carbonic acid. That's soda water, basically. Do YOU think that would work? (Hint: NO!)

The oxalates of Nd and Fe are basically insoluble. It's a recipe for stalled reaction/big mess.

Go down the hardware store and get some 'muriatic acid' (HCl) or toilet drainer (H2SO4).


http://i.word.com/imedical/permanganic%20acid
It does by the way




Elements Collected: 19/81 (Excluding all radioactive, using placecard for those)

Any tips or good sources are welcome.
View user's profile View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 26-5-2015 at 13:51


Making permanganic acid is an extremely difficult endeavor, and it's not even stable for long in water. The use of oxalic acid works by complexing the iron away as the soluble tris(oxalato)ferrate(III) complex as the neodymium precipitates as the normal oxalate.



At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2015 at 14:11


Quote: Originally posted by DalisAndy  


http://i.word.com/imedical/permanganic%20acid
It does by the way


A word of advice: medical dictionaries aren't the beez knees for looking up chemical stuff, you know? :cool: <=== that's a picture of a doctor in cool shades, nodding approvingly, BTW...


[Edited on 26-5-2015 by blogfast25]




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2015 at 14:13


Quote: Originally posted by Brain&Force  
Making permanganic acid is an extremely difficult endeavor, and it's not even stable for long in water. The use of oxalic acid works by complexing the iron away as the soluble tris(oxalato)ferrate(III) complex as the neodymium precipitates as the normal oxalate.


Errrmmm... except that oxalic acid won't oxidise Fe to Fe(III). So that separation method I proposed (and which works) only works AFTER the Fe has been oxidised to Fe(III).




View user's profile View All Posts By User
DalisAndy
Hazard to Others
***




Posts: 129
Registered: 8-5-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 09:32


Quote: Originally posted by blogfast25  
Quote: Originally posted by Brain&Force  
Making permanganic acid is an extremely difficult endeavor, and it's not even stable for long in water. The use of oxalic acid works by complexing the iron away as the soluble tris(oxalato)ferrate(III) complex as the neodymium precipitates as the normal oxalate.


Errrmmm... except that oxalic acid won't oxidise Fe to Fe(III). So that separation method I proposed (and which works) only works AFTER the Fe has been oxidised to Fe(III).


So using sulfric then oxalic would separate the Neodynium? Since Fe is in the +2 oxidation state




Elements Collected: 19/81 (Excluding all radioactive, using placecard for those)

Any tips or good sources are welcome.
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 27-5-2015 at 09:45


It would, as I can attest to, but now you have to deal with the neodymium oxalate. So far, mine's resisted H2SO4, HCl, and even a mix of H2SO4 and NaNO3. Good luck to ya.



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 09:48


Once again I'd recommend you read this thread in its entirety. Many of your questions have been answered right here. I know it's long; It's a complicated process. It's worth it to learn as much about it as possible if you're serious about pursuing this project.
View user's profile Visit user's homepage View All Posts By User
DalisAndy
Hazard to Others
***




Posts: 129
Registered: 8-5-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 12:14


Does neodymium and other rare earths have black light florescent properties?



Elements Collected: 19/81 (Excluding all radioactive, using placecard for those)

Any tips or good sources are welcome.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 12:35


Quote: Originally posted by DalisAndy  
Does neodymium and other rare earths have black light florescent properties?


Also in the thread.

Also here:

http://en.wikipedia.org/wiki/Neodymium%28III%29_chloride




View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 27-5-2015 at 12:38


Has anyone successfully isolated Nd yet ?

There is a tiny vial of Neodymium Sulphate somewhere in the lab as i recall ...




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 13:02


Quote: Originally posted by aga  
Has anyone successfully isolated Nd yet ?

There is a tiny vial of Neodymium Sulphate somewhere in the lab as i recall ...


Compound yes (sulphate), metal no. Re. latter, MrHomeScientist is the 'Amundsen' of that race here on SM.




View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 27-5-2015 at 13:47


Huh ?

I followed some instructions in this thread around page 4000 or so and have had some nice lilac powder in a vial for many months.

That sample even survived the last Cull (to get the vials back) as the colour is rather nice.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 13:51


Quote: Originally posted by aga  
Huh ?



Listen, I've had 3 Chimay's and I'm not drunk yet. Try and keep up! ;)




View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 27-5-2015 at 14:15


In a universe far, far a way, a long, long time ago, ISTR that it began with some magnets in an acid ...

One appears to have made NdSO4 simply following something (i forgot what) in this thread.

Lilac powder awaiting further instructions.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 14:24


Quote: Originally posted by aga  


Lilac powder awaiting further instructions.


There are two Nd sulphates. One's nice ruby red crystals, the other a sandy, lilac powder. We don't know what causes the difference. Be a trailblazer! :D

Hint: I think it's hydration. Not sure though... The easiest way would be to determine sulphate content of both 'varieties'.


[Edited on 27-5-2015 by blogfast25]




View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 27-5-2015 at 14:27


Quote: Originally posted by aga  
Lilac powder awaiting further instructions.

1. Leave in vial to look pretty.
2. Start work on Lanthanum from pool phosphate remover.
3. Obtain another vial with pretty crystals.
4. Copy mrhomescientist's beautiful and highly effective apparatus
5. Come in second with a better yield on the Nd race
6. Win the La race.
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 27-5-2015 at 14:41


7. Get some more beers and just post nonsense.

Ok. sounds like a Plan.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 14:53


8. Look up protocol for BaSO4 gravimetry



View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 27-5-2015 at 16:18


I would also like to add that the pink oxalate seems completely resistant to a mixture of elemental bromine and sulfuric acid as well.
Running out of ideas to dissolve this thing...




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 16:38


Quote: Originally posted by elementcollector1  
I would also like to add that the pink oxalate seems completely resistant to a mixture of elemental bromine and sulfuric acid as well.
Running out of ideas to dissolve this thing...


Random chemical mixing won't get you anywhere. There's nothing bromine can do here.

Calcine the oxalate to oxide. Then treat with boiling 95 % (at least) H2SO4. Or fuse with NaHSO<sub>4</sub>.

[Edited on 28-5-2015 by blogfast25]




View user's profile View All Posts By User
DalisAndy
Hazard to Others
***




Posts: 129
Registered: 8-5-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 17:28


Quote: Originally posted by blogfast25  
Quote: Originally posted by aga  


Lilac powder awaiting further instructions.


There are two Nd sulphates. One's nice ruby red crystals, the other a sandy, lilac powder. We don't know what causes the difference. Be a trailblazer! :D

Hint: I think it's hydration. Not sure though... The easiest way would be to determine sulphate content of both 'varieties'.


[Edited on 27-5-2015 by blogfast25]

Ummm if they are crystals, shape can be determined by dissolving them and letting them solidify on a sting. Like borax ornaments




Elements Collected: 19/81 (Excluding all radioactive, using placecard for those)

Any tips or good sources are welcome.
View user's profile View All Posts By User
DalisAndy
Hazard to Others
***




Posts: 129
Registered: 8-5-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 17:36


Quote: Originally posted by blogfast25  
Quote: Originally posted by elementcollector1  
I would also like to add that the pink oxalate seems completely resistant to a mixture of elemental bromine and sulfuric acid as well.
Running out of ideas to dissolve this thing...


Random chemical mixing won't get you anywhere. There's nothing bromine can do here.

Calcine the oxalate to oxide. Then treat with boiling 95 % (at least) H2SO4. Or fuse with NaHSO<sub>4</sub>.

[Edited on 28-5-2015 by blogfast25]


Dude, oxalates decompose easily. Go look it up, like I did today. or you could use Lithium in ethanol (or what ever non-polar solvent you have). or when in doubt electrolysis, of it's sulphate form.




Elements Collected: 19/81 (Excluding all radioactive, using placecard for those)

Any tips or good sources are welcome.
View user's profile View All Posts By User
DalisAndy
Hazard to Others
***




Posts: 129
Registered: 8-5-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2015 at 17:45


I don't get why we haven't created a location to consolidate knowledge for projects? I mean like log all expirements done, so others can test it



Elements Collected: 19/81 (Excluding all radioactive, using placecard for those)

Any tips or good sources are welcome.
View user's profile View All Posts By User
 Pages:  1  ..  17    19    21  ..  24