Detonationology
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
Making Platinum Electrodes
For several months now, I have been quite interested in making a chlorate and perchlorate cell; however, I have been deterred by the cost of platinum
and platinum elecroplated electrodes. What is the most viable route to electroplating platinum onto copper or titanium strips? What Pt salt is most
accessible, lowest cost and yields the most metallic platinum?
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
I think hexachloroplatinic acid is the go to candidate for this sort of reaction, if I remember right. Your answers may lie somewhere in the
Technochemistry subforum!
|
|
jock88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 505
Registered: 13-12-2012
Member Is Offline
Mood: No Mood
|
|
By the time you purchase enough Pt salts to make the anode (and probably not succeed in making the thing anyways) you will have a Pt anode purchased.
|
|
szuko03
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 188
Registered: 3-4-2015
Location: USA
Member Is Offline
Mood: No Mood
|
|
It just seems that with perchlorate being so cheap its almost not worth it. I understand that simply obtaining something is why people do things but
Platinum is pricey and not something I would want to buy to experiment with I mean not until I have done the same types of experiments with less
costly materials.
Also if someone can get precious metal salt that yields a greater monetary value of its elemental form after extracting at a consumer level I want to
be the first to know please
Chemistry is a natural drive, not an interest.
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
It is not straightforward to get a good plating. Someones struggles with this have been documented on this forum before IIRC.
Furthermore, you will need an excess of the solution to make a plating bath large enough to submerge your anode and avoid depleting it too rapidly
while plating (you'll want the composition of the bath to remain more or less constant).
If you are just after the (per)chlorate as cheaply as possible, don't take this route. The amount of money you will spend setting up and perfecting
the process will afford you several ready-made anodes.
Its a nice challenge though.
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
papaya
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 615
Registered: 4-4-2013
Member Is Offline
Mood: reactive
|
|
It's also should be possible to make "clad" Pt anodes, if you own some length of Pt wire (from some type of thermocouples). Pt is soft so it'll be
possible to hammer the wire into some kind of foil and then everything is clear I think. One trouble will be Pt's high resistiance, but this one could
overcome with shorter pieces of wire all connected to a common joint.
[Edited on 5-5-2015 by papaya]
|
|
Detonationology
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
It is certainly a costly gamble to attempt to make my own electrodes, indeed. I want to be able to make my own KP without having to rely on online
pyro suppliers, but I suppose that the best bet would be to keep my eyes out for a decently priced anode on ebay (unless someone can inform me of a
more economical and reputable source).
|
|
jock88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 505
Registered: 13-12-2012
Member Is Offline
Mood: No Mood
|
|
An old Pt crucible is the way to go for a serious anode imo.
http://www.sciencemadness.org/talk/viewthread.php?tid=5050&a...
post of 30/12/11
|
|
hyfalcon
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Paint and bake your Pt salts onto your titanium substrate and add some Ru salts in along with it.
|
|
Detonationology
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
How thick must the Pt plate layer be in order to be effective? What is the approximate minimum amount of Pt needed per square inch in order to have a
decent anode that isn't going to smudge off after 1 use?
|
|
hyfalcon
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Read grasshopper:
http://www.sciencemadness.org/talk/viewthread.php?tid=9783
[Edited on 6-5-2015 by hyfalcon]
|
|