How to TOTALLY dissolve a solid


Hi there

I'm currently working with a team in a lab to test catalysts. We are trying to dissolve a catalyst composed mainly by Al, Zn and Cu. We analyzed this thing with XRD and XRF and the latter showed that only 80% of it was composed by metal oxides. The guy told me that there was a 20% of "something" but he didn't know what. We wanted to know exactly if there was more inside and so we tried to dissolve it in acids in order to later analyze it with AAS.

We thought that a simple acid digestion would have been enough, but it seems some inert material is in there. We thought of silicon dioxide or a stable allumina and so we tried dissolving it in HF but with no results. We couldn't dissolve this thing.

The solid is an Al, Zn, Cu mixed oxide (by XRD patterns it looks like hydrotalcite phase) with, maybe, aluminium magnesium carbonate hydroxide hydrate. The peak relative to the latter also fits with the graphite one.

We tried to dissolve it in:
1) hot aqua regia x4h under reflux: there was a very little bubbling in the beginning, most likely some carbonate decomposing to CO2 and H2O. The other bubbling was HNO3 decomposing to red NOx fumes. A fine dark suspension was obtained. It got filtered and washed with water. I'll weigh it next week.
2) Hot HNO3 x4h under reflux (EPA method 3050B): only a little bubbling was observed in the beginning just like above, then nothing at all. Even the vapours were very clear and transparent, no formation of red NOx (so no oxidation occurring). This was followed by the addition of H2O2 30%, with nothing much happening. The only bubbles were due to H2O2 decomposing at 100°C I think, since nothing happened when it was added to the cold solution. Everything was evaporated and a viscous black "thing" was obtained (looked like some heavy MW carbon compound).
3) Hot HF for 2h: only an even smaller bubbling could be observed. Most of the fumes coming out were HF vapours. This was followed by the addition of HNO3, with no reaction occurring, and later by H2O2 30%, that just decomposed. Everything was evaporated and a fine powder of the same color of the starting material was obtained. It lost 60% by weight though.
4) Hot solution of saturated NaOH followed by the addition of H2O2 30% for 1h: nothing at all happened. The solution just got dirty and the H2O2 decomposed.

Apparently there is a 20% of "something else" but we are running out of options. We couldn't dissolve the solid even in those conditions. If it was SiO2 or Al2O3, it should have dissolved in HF (1g in 15ml HF) and if it was any other metal oxide, the HCl/HNO3 mix should have dealt with it nicely on its own but nothing. We can't get to dissolve this stuff.

Also, if there was some organic compound, it should have been destroyed under those conditions. We were working at ca 100°C, under reflux, for hours with highly oxidizing substances.

We decided to try piranha solution on what remained from the HNO3 acid digestion (method 2) to see if it can get further dissolved, but we have little hope in this one since the HNO3/H2O2 mix didn't give good results. We'll try this next week.

What else could this shit be? It's a dark gray pellet that was grinded finely. Our only hope was HF but not even that could scratch the thing (the HF vapours scratched the fume hood glass tho, lol).

I had suggested them alkaline fusion but it looks like they never tried it in their life and weren't much convinced (they made me use HF tho, which is more of a bitch).

We could try TGA on this thing, in order to see if there is some organic stuff in it. We didn't try organic solvents, so that could also be an option. If it's some polymer, perhaps that would help a bit.

Do you have any suggestion on how to totally dissolve this stuff? (EPA method 3052B assures total dissolution of everything with a microwave digetion in HNO3/HF mix at 180°C and 25bar but the microwave apparatus has been fucked up for 2 months already and I don't think they have appropriate vessels for it anyways.

Thanks for your attention
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 20-3-2015 at 10:50


Quote: Originally posted by Metallus  

I had suggested them alkaline fusion but it looks like they never tried it in their life and weren't much convinced (they made me use HF tho, which is more of a bitch).


You might try this alkaline fusion from Holtzclaw et al, College Chemistry with Qualitative Analysis, 7th ed:

"Fusion with Sodium Carbonate Silicates and certain oxides and calcined salts may not be taken into solution by treatment with acid or Na2CO3 solution or by reduction with zinc. Fusion with Na2CO3 is effective with many of these substances. Transfer the residue remaining after zinc reduction of silver halides to a small nickel crucible. Add to the residue 100mg of anhydrous Na2CO3, about half as much K2CO3, and a few mg of NaNO3. Place the cruible in a small clay triangle and heat it in the hot flame of a Meker burner until the mixture fuses. Cool the crucible, add 1 ml of water, and warm the mixture until the solid mass has disintegrated. Separate the mixture and reserve the solution. Treat the residue with 8 drops of 6M HNO3 and warm in the hot water bath for a few minutes. Separate and add this nitric acid solution to the original solution. Analyze the solution for cations."




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 20-3-2015 at 11:01


I once assisted with the analysis of chromite rich mineral samples. They needed to be digested completely into solution for AAS analysis, but the conventional HF/HNO3/HClO4 methodology failed.

What worked well was digesting it in molten sodium peroxide in zirconium crucibles over a torch flame, swirling with tongs. I don't have the exact procedure available anymore, but you aught to be able to find it in the literature.




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 20-3-2015 at 11:04


BTW, is this a low-temperature water gas shift or methanol from H2/CO/CO2 catalyst?



Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
WGTR
National Hazard
****




Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 20-3-2015 at 11:07


Fusion with sodium bisulfate in a test tube, or with molten alkali hydroxide in a nickel crucible (or something). I dissolved calcined TiO2 in sodium bisulfate here:
https://www.sciencemadness.org/whisper/viewthread.php?tid=27...

Later in the thread, I ran some EDS spectra of glass:

https://www.sciencemadness.org/whisper/viewthread.php?tid=27...

This latter thing is part of my job, and I generally don't do freebies with that. It would have to go through my employer.
View user's profile View All Posts By User
Metallus
Hazard to Others
***




Posts: 116
Registered: 16-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 20-3-2015 at 11:17


Quote: Originally posted by deltaH  
BTW, is this a low-temperature water gas shift or methanol from H2/CO/CO2 catalyst?

Yes, more precisely for the high temperature shift.

EDIT
Anyways, I just did a bit of research and in some catalysts of this type it is stated that they add an inert material like MgAl2O4.

If this was the case, how am I supposed to dissolve it? I'm a fan of alkaline fusion since when I saw it destroying glass at a faster rate than HF, but these guys just throw sulfuric and nitric acid at everything, hoping that it dissolves. How do I get them to understand that this is actually a viable method?

Once one of them was trying to remove fused V2O5 stuck in a test tube. I told him to try with some diluite HCl and he was like "huh, I'll see". Not much convinced, he asked an older dude who told him "Try sulfuric and nitric acid to oxidize it and remove it"... but what the fuck, V2O5 is already in its maximum oxidation state, it's non-sense using an oxidizing solution... and in fact it didn't work. The guy later tried HCl and wonder what...



[Edited on 20-3-2015 by Metallus]

[Edited on 20-3-2015 by Metallus]
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1698
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 20-3-2015 at 11:45


I was thinking fusing it with sodium carbonate, boric acid or perhaps a borate. I know borate is used for xrf-analysis of cement and it's raw materials, I think it was either lithium thetraborate or metaborate.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3621
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 20-3-2015 at 13:29


I am a novice so maybe this is rubbish,

if I wanted an inert substrate I might use something like asbestos,
I do not know how to test for that but you may.

Can you get a spark spectrum, that may give a clue to the composition?
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 21-3-2015 at 11:32


Low-temperature WGS :o wow, thought those were traditionally iron-based and copper used for the low-temperature shift. Crap... I'm getting old :mad:



Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
Metallus
Hazard to Others
***




Posts: 116
Registered: 16-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 21-3-2015 at 19:45


Quote: Originally posted by deltaH  
Low-temperature WGS :o wow, thought those were traditionally iron-based and copper used for the low-temperature shift. Crap... I'm getting old :mad:

Catalysts for the High temperature shift are traditionally iron/chromium based.

We are trying to synthetize a chromium free catalyst containing copper that doesn't suffer the sintering at the high temperature. In the past they've actually managed to produce such chromium free active catalyst, we are just trying to improve it further. But ye, if you look into literature, you'll find out that there have been developments in the WGS.
View user's profile View All Posts By User