Author: Subject: Issues with Rochelle's Salt Synthesis
nlegaux
Hazard to Self
**




Posts: 93
Registered: 28-11-2014
Location: East Tennessee
Member Is Offline

Mood: No Mood

[*] posted on 5-1-2015 at 13:36
Issues with Rochelle's Salt Synthesis


The past few days I have tried twice to synthesize and grow crystals of Rochelle's salt. My procedure is as follows:

- Create 80ml of saturated Potassium Bitartrate solution (I used Cream of Tartar because the MSDS claims it is 99.5% pure) in a 100ml beaker
- Add small amounts of Sodium Carbonate (created by decomposing Sodium Bicarbonate) until gas is no longer evolved
- Boil solution down to less than 20ml and allow to sit overnight

The first time I attempted the synthesis, no crystals formed. I let it sit 2 days, and at the end of the second day mold began to grow in the solution, so I disposed of it. The second time I attempted the synthesis, large dendritic crystals grew up the sides of the beaker. By the end of the next day, a mass of small needle-like crystals had grown throughout the solution. I still have the solution/crystals, but they do not seem consistent with what I have read about Rochelle's salt/Potassium Sodium Tartrate. Any ideas on what I may be doing wrong and/or any improvements to my procedure you can think of?

Sorry if this would fit better in the beginnings section...

Thank you,
nlegaux
View user's profile View All Posts By User
Pasrules
Hazard to Self
**




Posts: 78
Registered: 4-1-2015
Location: Yellow Cake Deposit
Member Is Offline

Mood: Lacking an S orbital

[*] posted on 5-1-2015 at 13:40


Just a simple trick. when you try for a third time use the crystal from your second run as a seed to encourage crystal formation.
And be very gentle the moment you let it cool, just sit it on the bench and let it do it's thing.

[Edited on 5-1-2015 by Pasrules]




Atropine, Bicarb, Calcium.
View user's profile View All Posts By User
DJF90
International Hazard
*****




Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline

Mood: No Mood

[*] posted on 6-1-2015 at 00:17


The data I found states that potassium bitartrate has an aqueous solubility of 6 mg/mL. Given the vastly improved solubility of Rochelle salt, you may be much better off slurrying the bitartrate with a stoichiometric amount of e.g. 2M hydroxide solution. Given the acid-base reaction, the solids should dissolve over time to give a full solution of rochelle salt. Any undissolved matter can be filtered off before concentration and crystallisation. It may be advantageous to use a stronger caustic solution (less to boil away later...) but you'd have to play around with it yourself.