Author: Subject: Aluminum and copper sulfate something wired
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 4-2-2005 at 18:48
Aluminum and copper sulfate something wired


I was making some powdered copper from copper chloride and aluminum foil as I added the al it started to bubble cl off witch doesn’t make since so how could it be if any thing it would be hcl however there was sodium sulfate in so may be the hcl in the solution made sodium bisulafate and cl



View user's profile Visit user's homepage View All Posts By User
Mumbles
Hazard to Others
***




Posts: 436
Registered: 12-3-2003
Location: US
Member Is Offline

Mood: Procrastinating

[*] posted on 4-2-2005 at 22:41


Aluminum Chloride hydrolyses to HCl and Al(OH)3 by the equation:

AlCl3 + 3 H2O ---> Al(OH)3 + 3 HCl

This could be a source. This reaction proceeds pretty slow however. The sodium sulfate could very well have something to do with it though. I can't really think up an equation, but I suppose there is something out there.
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
darkflame89
Hazard to Others
***




Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline

Mood: No Mood

[*] posted on 5-2-2005 at 01:08


Indeed i noticed the strange reaction as well. There were bubbles of gas evolved when i placed aluminium foil into copper(II) sulphate.
But i did not test the gas, and so could not verify the gas's identity at the momoent of time.




Ignis ubique latet, naturam amplectitur omnem.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 5-2-2005 at 03:13


Probably hydrogen.
2Al +6H2O --> 2Al(OH)3 + 3H2
View user's profile View All Posts By User
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 5-2-2005 at 08:56


its not H2 it was Cl2 i couled smell it and it was yellow
View user's profile Visit user's homepage View All Posts By User
Mumbles
Hazard to Others
***




Posts: 436
Registered: 12-3-2003
Location: US
Member Is Offline

Mood: Procrastinating

[*] posted on 5-2-2005 at 15:30


I need some clarification. Did you use Copper Chloride, or Copper Sulfate? The title says one thing, but your post says another. I assume you meant Copper Chloride, as otherwise there would be no possible way for chlorine.
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 5-2-2005 at 15:42


Check the pH of your copper salt solution. I would suspect it is acidic (salt of strong acid and weak base). If it is acidic then H2 would be a good guess.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 6-2-2005 at 06:35


Production of chlorine in the presence of as strong a reducing agent as aluminium would be remarkable.
If the solution gets hot enough then HCl from AlCl3 +H2O is possible.
View user's profile View All Posts By User
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 6-2-2005 at 09:52


Is it possible to add HCl to NaSO4 to make NaHSO4 and Cl?



View user's profile Visit user's homepage View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 6-2-2005 at 10:38


No. If anything, this would happen:

Na<sub>2</sub>SO<sub>4</sub> + HCl <--> NaHSO<sub>4</sub> + NaCl

To liberate chlorine, you need a strong oxidizer in a basic environment.
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1153
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 6-2-2005 at 14:31
Soluble


Chlorine is ALOT more soluble in basic solutions than in neutral or acidic. The gas is more likely hydrogen and this is evolve from the protinated chloride ions in solution. Copper Chloride is quite acidic and makes a good dipping sauce.:o:o Errr... I mean it hydrolisizes in water to form small amounts of HCL



Fellow molecular manipulator
View user's profile View All Posts By User
Mumbles
Hazard to Others
***




Posts: 436
Registered: 12-3-2003
Location: US
Member Is Offline

Mood: Procrastinating

[*] posted on 7-2-2005 at 14:06


I think of anything you have some gas released that has some, or is entirely HCl. HCl and Chlorine to smell rather similar. One is more burning, and one is more clean smelling I suppose you could describe it. In small doses it is sometimes hard to tell with the chlorine forming HCl with moisture in your nose.