Separation of metals from Non Lead Solder


I was hoping there was a method for separating the menials in non lead solder. The main metals in solder are Tin, coper indium and silver. The solder I have is Tin and silver. I guess That if I wanted tin I could just use it as is but can I remove the silver? Maybe adding nitric acid to make tin oxide and silver nitrate?

[Edited on 28-9-2014 by SimpleChemist-238]
View user's profile View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 28-9-2014 at 12:22


Then you'd want to remove the silver by adding copper to the silver nitrate to get silver metal. Or you could add salt to precipitate the silver as AgCl.

[Edited on 28.9.2014 by Brain&Force]




At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
SimpleChemist-238
Hazard to Others
***




Posts: 147
Registered: 28-9-2014
Member Is Offline

Mood: Chlorine Trifloride Flame Thrower

[*] posted on 28-9-2014 at 15:39


awesome thanks
View user's profile View All Posts By User
SimpleChemist-238
Hazard to Others
***




Posts: 147
Registered: 28-9-2014
Member Is Offline

Mood: Chlorine Trifloride Flame Thrower

[*] posted on 28-9-2014 at 17:38


I am going to try dissolving the alloy in HCl and whats left over is silver.
View user's profile View All Posts By User
TheChemiKid
Hazard to Others
***




Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline

Mood: No Mood

[*] posted on 28-9-2014 at 17:43


There will also be copper left. It may be tough to see because it a very fine precipitate.
View user's profile View All Posts By User
SimpleChemist-238
Hazard to Others
***




Posts: 147
Registered: 28-9-2014
Member Is Offline

Mood: Chlorine Trifloride Flame Thrower

[*] posted on 29-9-2014 at 03:42


how well does it act as a electrode
View user's profile View All Posts By User
Bezaleel
Hazard to Others
***




Posts: 444
Registered: 28-2-2009
Member Is Offline

Mood: transitional

[*] posted on 29-9-2014 at 09:14


As far as I remember, dissolving solder in nitric acid, produces hydrated SnO, not Sn2+. This is precipitated as a white to yellowish rather voluminous precipitate, called tin butter (SnO.xH2O). I used this procedure to separate tin and lead from a piece Sn/Pb solder wire, the lead remaining in solution.

I imagine the same to happen with alloys of tin and silver, the silver remaining in solution.
View user's profile View All Posts By User
SimpleChemist-238
Hazard to Others
***




Posts: 147
Registered: 28-9-2014
Member Is Offline

Mood: Chlorine Trifloride Flame Thrower

[*] posted on 29-9-2014 at 10:25


Cool, thank you for the info.
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1482
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline

Mood: Good

[*] posted on 29-9-2014 at 11:48


https://www.youtube.com/watch?v=G1sq4hnrBgM
"Pretty Tin crystals grown by electrolysis of Tin(II) Chloride solution.
The video is in real time."


https://www.youtube.com/watch?v=Af9GAUYDrlQ
"in the upper lefthand corner (anode) is a chunk of 95/5 tin/antimony electrical solder wrapped in filter paper to catch the bits of antimony that drop off as the tin dissolves"
View user's profile View All Posts By User