Test for genuine Turquoise?
Can anyone think of a very simple chemical test to confirm real turquoise from fake dyed stones, howlite etc. Turquoise is aluminum phosphate with
small amounts of copper so I was thinking a phosphate test of come kind would do the trick
any ideas?
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Copper test would probably be more suitable.
What about the standard mineral tests? Scratch plate, Mohs hardness, etc.?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
D4RR3N
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 271
Registered: 9-1-2007
Member Is Offline
Mood: No Mood
|
|
Testing hardness requires equipment, I just want some test that will identify if copper or phosphate is present.
I just want to crush a small sample into powder and drip a solution on it and get a positive or negative result.
|
|
HgDinis25
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 439
Registered: 14-3-2014
Location: Portugal
Member Is Offline
Mood: Who drank my mercury?
|
|
Actually, testing hardness could only require a piece of glass, a nail, a finger nail, and some knowledge.
Anyway, heat it up with concentrated Sulfuric Acid in a test tube. If it's Copper Phosphate it should form an equilibrium, thus coloring the solution
blue. Watch out for phosphric acid fumes.
|
|
D4RR3N
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 271
Registered: 9-1-2007
Member Is Offline
Mood: No Mood
|
|
Fake turquoise is dyed blue so it may turn the solution blue anyway?
Perhaps a phosphate test would be more accurate since turquoise is the only gem stone to contain it whilst copper may be common to many.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
No, concentrated sulfuric acid would likely destroy the dye.
Copper is not very common in gemstones - come to think of it, I can't think of any other major gems containing copper... Unless as trace impurity.
Azurite maybe? But it's a very different shade than turquoise...
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
D4RR3N
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 271
Registered: 9-1-2007
Member Is Offline
Mood: No Mood
|
|
Malachite contains copper in a high degree, formula for Turquoise is actually CuAl6(PO4)4(OH)8ยท4H2O it is not copper phosphate as someone above
stated.
so basically I heat some crushed turquoise with conc sulphuric acid and if it turns blue its genuine turquoise?
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Pretty much, yeah. Dyed howlite would just dissolve to a clear solution (destruction of dye and dissolution of the Ca/B/Si oxyhydroxide).
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
If I'm reading things correctly, unhardened mild steel will scratch howlite but not turquoise.
If I was looking for something to dye howlite, I might use a copper based dye like monastral blue or even a solution of copper sulphate.
|
|
zed
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
A lot of fakes are actually mineral stuff, stuck together with resin. Touch the tip of a red hot pin to the backside of your purported turquoise.
If it melts, it's bogus.
|
|