Author: Subject: Decomposition of MEKP
harinis
Harmless
*




Posts: 1
Registered: 29-10-2004
Member Is Offline

Mood: No Mood

[*] posted on 29-10-2004 at 03:33
Decomposition of MEKP


Could any one tell me wat is the decomposition product of methylethyl ketone peroxide and acetyl acetone peroxide by thermolytic cleavage.I am looking into the application of these peroxides in UPR curing.Kindly help me.



Harini
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 29-10-2004 at 11:45


I am not sure I understand your question.
You are wondering how MEKP or acetylacetonperoxide reacts with a resin, and what sort of end products are formed (after polymerisation has completed)?
Well, there are numerous possibilities in the case of MEKP, i.e. the oxygen radical (there are potentially 4, but at least 2 radical oxygens per molecule MEKP) from each methylethylketone reacts with the polymer, or it forms the ketone etc etc. Ultimately you will have a mixture of things.