I have a 500ml glass bottle with a ground glass stopper that is around 3/4 full of 98% H2SO4, It's been sitting there for a good 3-4 years now and I
noticed that there are crystals forming around the stopper, is this normal? What would the crystals be?
H2SO4 is from unused battery electrolyte that was boiled down if that helps at all.
|
|
Hockeydemon
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 218
Registered: 25-2-2013
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Guest ![](images/xpblue/lastpost.gif) | I have a 500ml glass bottle with a ground glass stopper that is around 3/4 full of 98% H2SO4, It's been sitting there for a good 3-4 years now and I
noticed that there are crystals forming around the stopper, is this normal? What would the crystals be?
H2SO4 is from unused battery electrolyte that was boiled down if that helps at all. |
It is most likely sulfation which is a common battery deterioration. Did you perform a titration to determine it's concentration? If not then it is
likely it is less than 98% pure, and has contaminants from the battery.
|
|
Guest
Harmless
Posts: 8
Registered: 12-6-2013
Member Is Offline
Mood: No Mood
|
|
It was never in a battery, went straight from the bottle it was purchased in into a beaker, boiled until it reached over 330C and then poured into the
bottle it's in now.
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Is it sitting near a bottle of ammonia or an ammonia salt?
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
Pulverulescent
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 793
Registered: 31-1-2008
Member Is Offline
Mood: Torn between two monikers ─ "hissingnoise" and the present incarnation!
|
|
Additives in battery acid?
"I know not with what weapons World War III will be fought, but World War IV will be fought with sticks and stones"
A Einstein
|
|
Guest
Harmless
Posts: 8
Registered: 12-6-2013
Member Is Offline
Mood: No Mood
|
|
There have been two small bottles near it, one containing Potassium Hydroxide solution, the other containing Phosphoric Acid (I know acids and bases
shouldn't be stored together but when they were put in their current home i didn't have much choice due to space limitations), both are sealed in
screw top HDPE bottles, the phosphoric has some crystallisation around the outside of the bottle (no doubt from where i dribbled some while pouring
years ago). Several feet away there is a bottle of copper solvent containing ammonia however it's also sealed in screw top HDPE bottles. I'll try to
upload a pic. It's been a while since i've played around with chemistry and want to make sure it's not something that will give me a nasty surprise if
i open it.
|
|
Guest
Harmless
Posts: 8
Registered: 12-6-2013
Member Is Offline
Mood: No Mood
|
|
Picture
|
|
Endimion17
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
I'm pretty much certain those crystals on bottles of acids are salts of ammonia. Ammonia is a normal constituent of our atmosphere, which
concentration increases in areas of greater biological activity. After few years of sitting on a shelf, even relatively clean air will contribute to
crystals or fogging near the bottle opening.
Those crystals are especially prominent, and appear rather quickly (months), in areas where bottles of ammonia or volatile ammonia compounds are
stored, like most of the laboratories people usually encounter.
Of course, things will speed up if acids are stored in an old fashioned way, in old bottles with rather gritty ground glass joints that leak horribly.
I remember working for few hours a week in one lab where tons of such bottles were sitting on shelves, few of them containing nitric acid and most of
them containing aqueous metal salt solutions. There was always a decent smell of nitrous vapours lingering through the air. I'm sure the ppm levels
were through the roof. Luckily for me, I got the hell out of there after few months.
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Quote: | from where i dribbled some while pouring years ago). Several feet away there is a bottle of copper solvent containing ammonia however it's also sealed
in screw top HDPE bottles. I'll try to upload a pic. It's been a while since i've played around with chemistry and |
Ammonia vapour can slowly permeate through the HDPE. It could have accumulated over the years.
I always notice a smell around bottles of nitric acid, even professionally stored glass nitric acid bottles with an appropiate cap. If you touch any
of the glass bottles surrounding it, your skin picks up a characteristic smell which is different from the nitric acid/nitric oxide itself.
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i have seen similar effect on 5 litre 62% HNO3 'bottles' or whatever you can call them..
apparently something from the air is capable of reacting with it..
the place i saw this was in a hardware store where they also had ammonia standing around (25%) but very well sealed off, so it couldnt have been
that.. perhaps CO2 in air or something alike..?
there was literally needly crystals on the plastic, seemed like it had the same properties of aluminium nitrate
full plastic containers
|
|
annaandherdad
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 387
Registered: 17-9-2011
Member Is Offline
Mood: No Mood
|
|
This is discouraging. I had been hoping that the manufacturers of battery acid would have a motivation to sell pure acid, without additives or
impurities. (Maybe some do.) This would be an advantage over drain cleaner as a source of OTC sulfuric acid, which often seems to have carbon and
other impurities in it.
Any other SF Bay chemists?
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
It's easy enough to check if it's ammonium sulphate.
Wipe it off and add a strong base like NaOH.
If the mixture smells of ammonia then you know it was an amonium salt.
It's also possible that it will smell a bit fishy due to traces of methylamines in air being trapped by the acid.
|
|