Author: Subject: Metathesis of KClO3 from NaCLO3
binaryclock
Hazard to Others
***




Posts: 121
Registered: 9-4-2013
Location: Canada
Member Is Offline

Mood: Organic

[*] posted on 2-5-2013 at 22:00
Metathesis of KClO3 from NaCLO3


Hello:

I've recently created a batch of crystals of NaCLO3 that were in electrolysis cells for three days in a solution of NaCl.

After three days, I boiled the solution to remove any hypochlorates and then added the same amount of KCl to the mixture and allowed it to perform metathesis. Some crystals formed immediately and sank to the bottom. After a while I took the solution and put it in the freezer to about 0c. At 0c, almost half the beaker was filled with crystals so I harvested them by decanting the liquid solution and putting the crystals on filter paper to dry.

Once dry, when burned the flame was yellow/red. It was not purple like my KCl syth crystals. It seems that I have more NaCLO3 than KCLO3 in my yield from the NaCl cell. What did I do wrong here?

Now that I have about 40g in dry crystals, how should I best go about getting them converted to KClO3 crystals?

Thanks




Current Project: Playing with my new Laboy advanced distillery kit!
View user's profile View All Posts By User
chemcam
Hazard to Others
***




Posts: 423
Registered: 18-2-2013
Location: Atlantis
Member Is Offline

Mood: I will be gone until mid-september, on a work contract.

[*] posted on 2-5-2013 at 22:14


Even a small amount of NaClO3 contamination will discolor the flame of KClO3 you most likely have more K than Na so I would take advantage of their different solubilites and do a 0C water wash. You will lose some product but gain purity.



My YouTube Channel: ChemCamTV
IRC Channel: #sciencemadness @ irc.efnet.org
View user's profile Visit user's homepage View All Posts By User
binaryclock
Hazard to Others
***




Posts: 121
Registered: 9-4-2013
Location: Canada
Member Is Offline

Mood: Organic

[*] posted on 2-5-2013 at 22:23


Thanks for your reply. I'll try that tomorrow and see how it goes. I wasn't aware that a small amount of NaCLO3 discoloured the flame.. thanks for the info!




Current Project: Playing with my new Laboy advanced distillery kit!
View user's profile View All Posts By User
ScienceSquirrel
International Hazard
*****




Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline

Mood: Dogs are pets but cats are little furry humans with four feet and self determination! :(

[*] posted on 3-5-2013 at 03:27


Sodium floods everything in flame tests, your product could be at 99% pure and the sodium would still show up.

http://chemistry.about.com/od/analyticalchemistry/a/flametes...
View user's profile View All Posts By User
binaryclock
Hazard to Others
***




Posts: 121
Registered: 9-4-2013
Location: Canada
Member Is Offline

Mood: Organic

[*] posted on 3-5-2013 at 05:26


Cool thanks for the link. Scumbag sodium :)





Current Project: Playing with my new Laboy advanced distillery kit!
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 3-5-2013 at 06:51


That's why many of us start with KCl when we want the end product for use in pyrotechnics. If the sodium is never there then it can't ruin the show!
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1379
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 3-5-2013 at 07:17


Fortunately, the solubilities of KClO3 and NaClO3 work in your favor:

1. good recovery
KClO3 solubility varies strongly with temperature and it is only moderately soluble in cold water, so the recovery of recrystallizations is quite good.

2. Big difference beteen solubility of NaClO3 and KClO3
NaClO3 is -very- soluble, even at low temperatures, so it is doable to get rid of even small impurities of NaClO3. For best results, use suction on filtration (buchner filter works very well) to remove recrystallisation liquor and wash once/twice with ice-cold water in the filter.




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 3-5-2013 at 08:21


There's a thread on converting NaClO3 (used to be in some weed killers) to KClO3 on this forum.



View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 3-5-2013 at 15:11


i would say even just using cloth for filtration and then squeezing it would be enough, a neat little tip is to take tissue paper, fold filter in half and suck the water out of both the insoluble and the filter with the dry tissue paper
this can be done with normal filter paper ofc.. very very handy especially if you can combine that with ether then you could do it in literally less than 10 mins

in short
squeeze out the liquid of the filter, or scrape the crystals onto tissue paper and let them dry, then you shouldnt need to purify it further by recrystallization




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User

  Go To Top