toothpick93
Harmless
*




Posts: 44
Registered: 26-2-2013
Member Is Offline

Mood: No Mood

[*] posted on 4-3-2013 at 05:27
Strange colour change Happening


So i was etching large bits of copper pipe which was pretty bardly corroded. I then had some small bits of copper so i thought to do a close up view and when i mixed the h2o + h2o2 solution with the hcl, well it made the solution turn brown. As the copper reacted with the solution, it changed to the green colour of copper chloride. so why the brown colour?


No pictures, only part of the video, just watch the first 5 seconds to see what i mean. Or spend 2 minutes watching the copper corrosion disolve :)
http://www.youtube.com/watch?v=HVWrlu68OO4&feature=youtu.be
View user's profile Visit user's homepage View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 4-3-2013 at 10:55


ive experienced the same thing, but didnt think further about it..
when i did it i wanted to etch some osmium (i believe it was?) from a long lightbulb
when adding the H2O2 it somehow bubbles alot and smells like chlorine (H2O2 + HCl > Cl2?) it should make some stronger etching solution, didnt work for me with HCl on copper and H2O2 added in, but there was the same bubbling tho no actual reaction with the copper as i remember..

but also with steel + unknown metal this effect / reaction occurs so i doubt its anything specific with the copper, tho it could of produced CuO to then react with the HCl again..




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
Mixell
Hazard to Others
***




Posts: 449
Registered: 27-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 4-3-2013 at 13:00


the CuCl2(-) anion (Copper I chloride dissolved in concentrated HCl) is brown, but you say that the brown color was formed without the copper? just HCl and H2O2? Is there a chance one of your reagents my be impure?

H2O2 can oxidize Cl-, but the solution should be just slightly greenish-yellow (barely noticeable), not brown...
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4319
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 4-3-2013 at 13:05


Quote: Originally posted by Mixell  
the CuCl2(-) anion (Copper I chloride dissolved in concentrated HCl) is brown, but you say that the brown color was formed without the copper? just HCl and H2O2? Is there a chance one of your reagents my be impure?

H2O2 can oxidize Cl-, but the solution should be just slightly greenish-yellow (barely noticeable), not brown...

I thought that it was CuCl4(2-) that was brown (Cu(I) is a d10 system, and isn't expected to be colourful). When you dissolve CuCl in HCl, you always get some of the Cu(II) ion forming, since there is some oxygen dissolved in the acid (unless you've degassed it), and the solution is exposed to air.

If you got brown when you first added the copper, and then that faded to green as the ratio of chloride to copper ions decreased, that would make sense...




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8011
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 4-3-2013 at 13:40


Quote: Originally posted by Mixell  
the CuCl2(-) anion (Copper I chloride dissolved in concentrated HCl) is brown, but you say that the brown color was formed without the copper? just HCl and H2O2? Is there a chance one of your reagents my be impure?

H2O2 can oxidize Cl-, but the solution should be just slightly greenish-yellow (barely noticeable), not brown...
Copper forms a mixed copper(I)/copper(II) complex in strong HCl.

CuCl2(-) is colorless, CuCl4(2-) is green/yellow, but when both are present (and that easily is the case in aqueous copper(I) solutions, which are exposed to air) then a very dark brown complex is formed.

Have a look at this: http://woelen.homescience.net/science/chem/riddles/copperI+c...

And especially the first part of the fifth experiment from that page may be interesting for you. In that experiment a colorless solution of copper(I) is oxidized by oxygen from air and a dark brown compound is formed.

http://woelen.homescience.net/science/chem/riddles/copperI+c...


[Edited on 4-3-13 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Mixell
Hazard to Others
***




Posts: 449
Registered: 27-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 4-3-2013 at 14:52


Yes, now that I think about it, the mixed-oxidation state compound sounds more logical.

But it doesn't explain the color if there was no copper present in the vessel or in the solution prior to the submergence of the pipe.