Make X-Aerogel
Can someone give me a clear guide to converting normal scilica aerogel into X-Aerogel like here?
They got a good guide on making scilica aerogel and how to sub-critically dry it, but I'd like somehelp for making it into X-Aerogel.
Thanks.
|
|
Diablo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 113
Registered: 17-9-2011
Member Is Offline
Mood: Autodidactic
|
|
http://www.aerogel.org/?p=1058
a guide to making x-aerogel
|
|
APO
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 627
Registered: 28-12-2012
Location: China Lake
Member Is Offline
Mood: Refluxing
|
|
I know I'd like to get better terms about the polymers used.
|
|
APO
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 627
Registered: 28-12-2012
Location: China Lake
Member Is Offline
Mood: Refluxing
|
|
Can I use any lighter polymer than polystyrene?
|
|