Plastic bottles for storing concentrated nitric acid?
Are there any common plastics that can store nitric acid around 98% conc.? I looked at several plastics and none were said to be resistant to it. I
was wondering because glass bottles aren't cheap and plastic bottles are so easy to come by.
|
|
kristofvagyok
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
98% HNO3 may ignite on contact with most plastics (PE, PS, HDPE, PP ect.). It could be stored in a PTFE bottle, but I think glass is much cheaper.
Save your money, but not on your safety.
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
I already stored 10 ml yellow fuming nitric, 98%+ (that was able to make nitril catch fire) In a 15 ml Nalgene polyethylene bottle with polypropylene
cap (the one that cost 3$ each) and it did a good job. After 8 month it was still ok. I think the heavy nalgene p.e bottle are surface fluorinated.
I never asked for this.
|
|
Vargouille
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 380
Registered: 16-4-2012
Member Is Offline
Mood: No Mood
|
|
Depends on your definition of "common". According to Harrington, the materials that will withstand (red) fuming nitric acid are Halar (a trademarked
plastic good to about 80C), PTFE (to about 175C), carbon, ceramic, 304 stainless steel (something I find rather odd, considering that 316 stainless is
unsuitable), and Hastelloy C. Incidentally, Viton has no data.
I'd suggest splurging on the glass bottles and some high-quality teflon-lined caps.
|
|
kristofvagyok
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
There was 50cm3 95% HNO3 in a glass bottle with a standard PE cap. The cap cracked after 2 week and just "died" a few days later. Just the NO2 fumes
was identified....
We've got several liter of 100% HNO3 and all is stored in polymer coated breaksafe glass bottles with PTFE caps and is kept in diatomeous earth.
I would not pour +95% HNO3 again in a bottle that could give up in any time, it could cause surprise in any time.
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
Sublimatus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 108
Registered: 8-6-2011
Member Is Offline
Mood: No Mood
|
|
One thing to consider is NO<sub>x</sub> gases building up inside of whatever container you use.
I recall the first time I synthesized HNO<sub>3</sub>, I stored it in a brown Boston round bottle with a PTFE lined plastic cap. I forgot
about it for a few months, and the next time I went to use it I noticed that the cap seemed cracked. I found this perplexing, since I couldn't
imagine how the acid fumes might have gotten past the liner to attack the cap.
Of course when I unscrewed the cap, a mist of NO<sub>x</sub> and nitric acid blew out around the mouth of the bottle as the pressure
equalized. I was rather surprised, since I hadn't considered that the cap was cracked due to internal pressure. In hindsight it's fairly obvious what
I had in my hands.
These days I have my nitric acid in a Schott Duran bottle with a more robust red PBT cap and PTFE liner.
The NO<sub>x</sub> gases may not be a concern for purified and commercial nitric acid. However, it's clearly something to think about
with homemade acid (mine was clear after synthesis, but with time has turned orange).
[Edited on 1/21/2013 by Sublimatus]
|
|
Nickbb
Harmless
Posts: 25
Registered: 6-12-2012
Location: 3rd dimension
Member Is Offline
Mood: something other than a chemistry pun
|
|
Thanks for all the replies... I guess it is best to stick with glass bottles, I like them better anyways and I just picked up several of them for a
dollar and a half at a organic grocery store (who knows why they sell them..) Also thank you for that piece of information there Sublimatus; I'll have
to remember to vent the bottle every now and then if I keep it around for long enough.
|
|