does anybody have an idea as to what happened?


hi,
today I took my dry K2CrO4 out of my evaporation dish (I made it from K2Cr2O7 and KOH) and when i washed the dish I got a big surprise!
the entire bottom of the dish was frosted! Could the KOH I used have caused this? i never heated it over 140*C. wouldn't it take a lot longer to do this?


evap dish.jpg - 181kB




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 31-10-2012 at 08:17


What's with the magical '140*C'?

Concentrated solutions of alkali metal hydroxides will eat glass anyway, how long was the KOH solution in contact with the glass for?

I've seen this happen a few times and have a got a few beakers in this kinda state.




"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 31-10-2012 at 08:20


3 days. whenever I was there I heated it. but when I was heating it i saw the temp. on my hotplate and it was mostly between 95-120* because temperature has to do with how fast an alkali attacks glass.



all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 31-10-2012 at 08:32


Naturally, as it is a chemical reaction between the KOH and the SiO2 in the glass to make potassium silicate.

Even at these temperatures you mention, a fair amount of dissolving would have taken place, particularly if the solution was concentrated.




"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 1-11-2012 at 11:51


Yes, Hexavalent is right. Even at room temperature, strong alkalies can attack glass. I once had a glass jar, which held a saturated solution of NaOH. I kept it in the jar for a week or so and after that week I could clearly see to what level the liquid was stored.

Never keep strongly alkaline solutions in glass for more than a few hours at room temperature and not more than a few minutes at higher temperature around 100 C.




The art of wondering makes life worth living...