Identify these bottles!
I might have had a thread on these a while back, but I'm still baffled by them, and I'd like to put them to use.
On eBay, I picked up a dozen bottles and lids that are MACHINED from solid PTFE - teflon. These are not PFA/FEP bottles.
These are sweet in every way but one - they are stained and carry a really funky odor, something very organic. I've tried cleaning them with all
sorts of hot mineral acids, pirhana fluid, everything. They are still stained and still smell. This blows my mind. I thought PTFE was just about
immune to attack, and can be cleaned with ease.
What are they for? My best guess is that they were part of some very expensive biotechnology machine. Perhaps they were filled with proteins, or
something to do with automated DNA analysis. The other option is the semiconductor industry, which might suck because of toxicity concerns.
I'm afraid to use them due to the possibility of contamination.

|
|
unionised
International Hazard
   
Posts: 5134
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I'm glad you are wearing gloves.
Those sorts of bottles are very expensive and so they only get used if there's nothing else that will do the job.
Whatever they were used for is probably rather corrosive (and the fact that it has stained the PTFE supports that).
I know it's not very green but the best suggestion I can give is that you take the lids off and leave them outside away from anyone for a while and
see if whatever it is dissipates.
Sunlight, oxygen, water and time makes for a pretty good cleaning agent.
|
|
Swede
Hazard to Others
 
Posts: 491
Registered: 4-9-2008
Member Is Offline
Mood: No Mood
|
|
It terms of actual "stuff" in the bottles, there is none. All that is left is the staining, and the smell. As mentioned, I tried peroxide, sulfuric
and nitric acids, soaking them overnight in the cleaners, and nothing has touched the staining.
I even sectioned one of them, and the stain itself extends into the PTFE a good mm or two, so it's not surface staining. I doubt that the stains at
least will ever come out, so I guess it comes down to "what good are they?"
I can potentially mount them in a lathe and turn them into PTFE beakers by boring out the cruddy part, but as original containers, they're probably
toast, which is sad, because they are neat little bottles and probably very expensive when new.
I think they were part of an automated machjine. They have the rigidity so that a machine can select, manipulate and open them, which is something
that a much more flexible PFA bottle couldn't deal with. And the lids have very specific grooves that look to accept a flanged opening mechanism.
|
|
Swede
Hazard to Others
 
Posts: 491
Registered: 4-9-2008
Member Is Offline
Mood: No Mood
|
|
Oh yes, just a little gloat - these were part of a huge lot of PTFE, PFA, and FEP lab bottles I picked up for something like $20. About 1/2 of these
were used, but the other half were brand spanking new, so now I have a nice collection of bottles from 100ml to 250ml that were probably $60 to $150
each when new. 


|
|
ScienceHideout
Hazard to Others
 
Posts: 391
Registered: 12-3-2011
Location: In the Source
Member Is Offline
Mood: High Spin
|
|
It sounds to me that they may have contained bromine... Is it bromine like? Have you tried cleaning it with sodium thiosulphate? Looks like the right
color for bromine...
hey, if you are reading this, I can't U2U, but you are always welcome to send me an email!
|
|
watson.fawkes
International Hazard
   
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Swede  | They are still stained and still smell. This blows my mind. I thought PTFE was just about immune to attack, and can be cleaned with ease.
| The chemical is inert, but the material is not impervious. Since PTFE doesn't take well to melt processing,
though it can be sintered under pressure. This, however, leads to less than 100% fill. But also, because PTFE is inert, even to itself, individual
grains don't bond much chemically, but rather mechanically, and with thermal cycling grain boundaries can open up transiently.
|
|
Ozone
International Hazard
   
Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline
Mood: Integrated
|
|
Bromine was my first instinct, as well.
O3
-Anyone who never made a mistake never tried anything new.
--Albert Einstein
|
|
woelen
Super Administrator
       
Posts: 8071
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I do not think it is bromine. Bromine stains are homogeneous, but as the picture shows, the stains in the bottle contain many little dark specks,
especially near the rim.
But of course, you can check easily. Just make a little bromine (e.g. take some chlorate, add to a solution of KBr or NaBr and then add some acid and
swirl, until you have a nice orange/red solution) and CAREFULLY compare the smell of the bromine with the smell of the bottles.
|
|
kristofvagyok
National Hazard
  
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
Doesn't look like bromine to me as well. I have worked a lot with bromine and never ever saw a colorination like this on the PTFE. It could be a
million else compounds what has az orangeish color...
Simply just don't care what is it, wash it out. Use acetone/methanol/KOH+isopropanol, just get it out. Non of these will damage the teflon, they will
just get out the gunk.
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
Swede
Hazard to Others
 
Posts: 491
Registered: 4-9-2008
Member Is Offline
Mood: No Mood
|
|
After a thorough cleaning, all identifiable solids are gone... long gone. All that remains is the staining and the smell. And if something is
embedded in the PTFE and volatile enough to be obvious to the nose, it's also going to interact with anything I store in there.
All I can think of is a protracted soak (weeks) in something potent, either 30% peroxide, or an organic solvent like acetone or MEK.
|
|
quinoxaline man
Harmless
Posts: 6
Registered: 26-7-2009
Member Is Offline
Mood: No Mood
|
|
Odor
Why not store in a vacuum desiccator under vacuum? Since the odor is noticible at atms. pressure, perhaps it will completely volatize under a high
vacuum.
Henry
|
|
Swede
Hazard to Others
 
Posts: 491
Registered: 4-9-2008
Member Is Offline
Mood: No Mood
|
|
That's a great idea, Henry, I'll give it a shot. Thanks!
|
|
feacetech
Hazard to Others
 
Posts: 163
Registered: 12-2-2007
Member Is Offline
Mood: No Mood
|
|
Looks kind of like "crude HFA" staining, from a SSP fertiliser plants scrubber process.
The Crude HFA can have a lot of iodine in it, this coupled with the HFA can stain PTFE like this.
[Edited on 7-10-2012 by feacetech]
|
|
Oscilllator
National Hazard
  
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
Tried sodium hydroxide? It is pretty good at cleaning. Other that that, the vacuum seems your best bet.
And yes, I am very jealous of your pot collection.
|
|
niertap
Hazard to Self

Posts: 76
Registered: 5-8-2011
Member Is Offline
Mood: hyper-conjucated
|
|
The specks might be from microscopic cracks created during the machining or small bubbles(defects) in the block they were machined from. the compound
could penetrate all of it slightly and the defects much more so. It really does seem like a small halide compound. it's high vapor pressure seems
evident of the staining where it escaped through the threaded lid.
Ignorance is bliss
Outliers in life are modeled by chemical kinetics
|
|
zed
International Hazard
   
Posts: 2285
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Well, you might be able to keep them intact, and hone them out with a brake cylinder hone attached to an electric drill.
Likewise, lathe attachments might be available that would allow you to re-machine the insides of your bottles.
Third, you might be able to Vacuum distill this stinky stuff out of your bottles. Think vacuum dessication + heat.
Fine lookin' bottles. Damn shame.
|
|