Metalworking Fluids
Somebody has information about Metalworking Fluids?
I am looking for it formula and ratio.
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Do you mean flux for soldering or brazing?
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
No,
Metalworking fluid (MWF) is the name given to a range of oils and other liquids that are used to cool and/or lubricate metal workpieces when they are
being machined, ground, milled, etc. MWFs reduce the heat and friction between the cutting tool and the workpiece, and help prevent burning and
smoking. Applying MWFs also helps improve the quality of the workpiece by continuously removing the fines, chips, and swarfs from the tool being used
and the surface of the workpiece. (Swarfs are the small pieces of metal removed from a workpiece by a cutting tool.)
[Edited on 28-5-2012 by Waffles SS]
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
tap magic is great for cooling especially tapping and drilling if you do hand drilling or tapping. if you're running lathes you'll need the water
soluble oil kind because it takes a whole lot just like those pictures you got there. tap magic also worked great for me when i was doing punching,
the old tap magic was better but they did away with it because rats and californians got cancer from it. good thing i live in Texas.
|
|
bquirky
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 316
Registered: 22-10-2008
Location: Perth Western Australia
Member Is Offline
Mood: No Mood
|
|
I use a mixture of motor oil, water and dish washing detergent. if you keep the system recirculating the fluid doesn't separate too much. it makes a
huge difference to the cuts as much through mechanical swaf removal as cooling and lubrication but man it sure dose make a mess
|
|
bquirky
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 316
Registered: 22-10-2008
Location: Perth Western Australia
Member Is Offline
Mood: No Mood
|
|
you can allso use oil and kerosene but i am nurvus about leaving the machine running evan momentarily un attended with that kind of flammable fine
mist floating around
Ive allready had a belt catch fire. flamabal collant is begging for trouble
[Edited on 28-5-2012 by bquirky]
|
|
Swede
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 491
Registered: 4-9-2008
Member Is Offline
Mood: No Mood
|
|
The number of cutting fluids is astronomical, and their formulas all vary. Synthetic, semi-synthetic, water soluble, bactericides and fungicides,
etc. Comes in flood, spray, mist varieties. The classic fluid consists of a soluble oil cut with water in varying proportions.
Are you trying to make your own?
Look at the MSDS for various cutting fluids and it'll give you an idea.
|
|
Waffles SS
Fighter
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 998
Registered: 7-12-2009
Member Is Offline
|
|
Quote: Originally posted by Swede ![](images/xpblue/lastpost.gif) |
Are you trying to make your own?
Look at the MSDS for various cutting fluids and it'll give you an idea. |
Yes,I want to make my own Metalworking fluid.
I tried one time and i was unsuccessful because after 2 week the odor of solution changed(due to bacteria and fungi activity)
One of my friend suggest me Bronopol(2-bromo-2-nitropropane-1,3-diol) but this cause corrosion in metals.
My Metalworking fluid made of 20% Emulsifier + 80% Industrial Oil.I add 5 part of this Metalworking fluid with 10 part of water and milky solution
obtained.I am looking for better formula and also better antibacteria ,antifungies (it should dissolve in oil)
[Edited on 28-5-2012 by Waffles SS]
|
|
bahamuth
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline
Mood: Under stimulated
|
|
Most of the "good" metal working fluids I have used is an oil base with large amounts of free ammonia in, which you mix with water at around 1-2% of
metal working oil:water.
If you want to make it yourself the oil have to be fairly light (short chain) and lubricating.
Once at metalworking class we were told to use used hydraulic oil, not a good idea I tell you, toxic oil smog everywhere...
Just buy a quart of the really good stuff, and it'll last a long time.
BTW I use a drop of the pure oil (not mixed with water) if I drill in high chromium alloys and works a little better than the mix IMO.
Any sufficiently advanced technology is indistinguishable from magic.
|
|