Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
is crystal any good for chemistry glass?
today my father asked me to clean 4 350$ crystal decanters because they were completely white inside, so i suggested H2SO4, and he thought it was a
great idea, so here goes:
#1: I mix sulfuric acid and water to dilute it a bit, and i waited for it to cool down, and poured it in... crack, broke into many pieces
#2: same thing
#3: it got nice and clean and i washed it all out and it went into the dishwasher
#4:it broke as well
so i collected all the shards and was wondering if i should give them to a glassblower to make a condenser? because it seems a pity to throw all this
expensive glass away.
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
bbartlog
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1139
Registered: 27-8-2009
Location: Unmoored in time
Member Is Offline
Mood: No Mood
|
|
Hm... at such a price I daresay i would have changed cleaning methods after the first one broke.
And if it won't withstand dilute sulfuric acid I don't think you can use it for lab glass.
The less you bet, the more you lose when you win.
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
well, we guessed that that was the only way, because we tried stones, lead shot, decalc, ball bearings,... and none worked. i think they cracked
because of the heat, because i don't think that H2SO4 will cause any glass to break, no?
[Edited on 1-5-2012 by Pyro]
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
Migratory
Harmless
Posts: 15
Registered: 30-4-2012
Location: Chemophobialand, California
Member Is Offline
Mood: No Mood
|
|
Just how hot did it get?
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
hot to the touch, it hurt to hold it for more than 5 seconds, id guess about 70 degrees.
it could be that they got non-visible cracks in them when they were jammed in a box, and they do go through a lot of shaking because of the engine.
but is crystal any good to get a condenser made?
[Edited on 1-5-2012 by Pyro]
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
Migratory
Harmless
Posts: 15
Registered: 30-4-2012
Location: Chemophobialand, California
Member Is Offline
Mood: No Mood
|
|
Yeah, sounds like they were damaged. All my crystal can survive boiling water. Anyway, it might be less expensive to buy the glassware than it is to
have it custom blown. It depends on your glassblower's rates.
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
i know about the resistance to heat of crystal, almost all our glasses are made of crystal.
ill check out the rates, i know a glassblower is handy for custom equipment.
it seems a pity to throw all that extremely expensive glass away...
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
Endimion17
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
The "white stuff" is calcium carbonate. Why on earth would you want to clean that with sulphuric acid, if the reaction gives insoluble calcium
sulphate?
Not only it's fairly easier and less expensive to obtain hydrochloric acid, but the product is pure solution of calcium and chloride ions that can be
rinsed away. How were you supposed to rinse away something that's essentially gypsum?
I think the glassware broke because of the formed precipitate in the scratches and pores.
Sulphuric acid is never used for cleaning limescale because it just makes the problem worse. HCl is for limescale, NaOH/detergent is for grease.
|
|
Neil
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
"Crystal ware" = by deffinition leaded glass.
Usless for anything other then cutting into pretty shapes that go tinnnnnnnnnnnnnnnnnnnng when you flick them.
If it is just Crystal then it could be leaded or unleaded but is likely a high K glass mixture. Not much use for it...
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
well it seemed to have an effect on the one that didnt break, it was completely white, now its clear.
it must have caused it to lift off the surface?
ok, ill throw it out.
thanks for the help