HDPE as a storage for Sulfuric Acid


I bought 5L of H2SO4, which arrived in what looks to be a HDPE container.

This amount of acid should take me, years to go through.

My question. 2-4 years from now, what if any damage to the bottle should I expect.





View user's profile Visit user's homepage View All Posts By User
woelen
Super Administrator
*********




Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 9-6-2010 at 01:27


If I were you I would rebottle it in glass bottles with decent plastic caps. I have no confidence in long-term storage of concentrated sulphuric acid in anything else than glass.

Fortunately, concentrated sulphuric acid does not fume, so, if it is stored in glas bottles, filled for 80% and the cap is tightly closed, then the cap will not be corroded by the acid, simply because the acid does not touch the cap.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
azo
Hazard to Others
***




Posts: 163
Registered: 12-2-2008
Member Is Offline

Mood: No Mood

[*] posted on 9-6-2010 at 02:51


hdpe containers are designed to biodegrade and in direct sunlight they start to break apart and cracks develop within 12 months , i think im with woelen i can only trust a good thick glass bottle :D



View user's profile View All Posts By User
rrkss
Hazard to Others
***




Posts: 193
Registered: 18-12-2009
Member Is Offline

Mood: No Mood

[*] posted on 9-6-2010 at 09:50


HDPE is supposed to be chemically compatable wtih concentrated H2SO4 however, my personal practice is to store diluted H2SO4 in HDPE and my concentrated stuff in glass. I'd rather be safe than sorry.
View user's profile View All Posts By User
iHME
Harmless
*




Posts: 30
Registered: 29-10-2008
Location: the arctic circle
Member Is Offline

Mood: No Mood

[*] posted on 10-6-2010 at 02:24


My labgrade concentrated H2SO4 came in a UHDPE bottle.
The bottle is already stained black/darkblue on the inside, but according to some online sources that is all that H2SO4 does to HDPE/UHDPE, it stains it.




It\'s a catastrophic success.
View user's profile View All Posts By User
Jimmymajesty
Hazard to Others
***




Posts: 153
Registered: 9-7-2009
Member Is Offline

Mood: No Mood

[*] posted on 10-6-2010 at 08:51


When I was younger I tried to store H2SO4 and HNO3 in PET bottle, now that I grew up I store the H2SO4 in HDPE and the nitric in glass bottle:)
View user's profile View All Posts By User
mycotheologist
Hazard to Others
***




Posts: 154
Registered: 16-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 21-4-2012 at 04:30


The hardware shops here sell 98% H2SO4 drain cleaner in HDPE containers. Heres a chart for HDPE chemical resistance:
http://pt.rexnord.com/products/guards/orange_peel_guards/hdp...
they list 98% H2SO4 as GG meaning it shows little or no damage after 30 days of exposure. The first G is at room temperature, the 2nd G is at 50C. I've had a HDPE bottle of 98% H2SO4 for over a year now and it hasn't degraded in any way from what I can see.
View user's profile View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 22-4-2012 at 05:09


I second the opinion about replacing the HDPE bottle with a good glass bottle/container... the HDPE container is just a temporary vessel since most "industrial" chemicals are used quite rapidly... I wouldn't leave it too long in there.

I've had recently an unfortunate experience with HDPE that surprised me (and scared me a little). I had this 1 liter white HDPE bottle that contained 99% isopropanol. Rencently as I was pouring some of it in a squirt bottle, the container literally shattered under the pressure of my fingers! Thank god it was only iso, because had it been sulphuric acid, I would have been one hell of a mess!

Since then, i've transfered most of my liquid reagents to glass reagent bottles, I feel safer that way, because there's no way any of these compounds will eat through glass.

The only exception are HCl, which comes in HDPE but I use it often so I never have a bottle for more than 6 months, and the solid NaOH and KOH bottles, which are HDPE but I hope will last long enough till I use 'em.

Robert