Mineral oil with density of 0.9 instead of 0.8?
For potassium separation I am searching for an oil slightly heavier than K metal which has a density of 0.86.
Which oil can I use for this? Most oils are 0.8.
|
|
zoombafu
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 255
Registered: 21-11-2011
Location: U.S.
Member Is Offline
Mood: sciencey
|
|
You could use canola oil, it has a density of .92 g/mL.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
"You could use canola oil"
briefly
http://en.wikipedia.org/wiki/Acyloin_condensation
|
|
entropy51
Gone, but not forgotten
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1612
Registered: 30-5-2009
Member Is Offline
Mood: Fissile
|
|
This would have been a good question for the short questions thread.
|
|
Mr. Wizard
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
More double bonded carbons, and longer chain length equals more density in general, as the ratio of C to H goes up.
|
|
metalresearcher
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 732
Registered: 7-9-2010
Member Is Offline
Mood: Reactive
|
|
So, candle wax (i.e. paraffin)?
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2687
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
The only thing that will make the density heavier than 0.9 would be more heteroatoms, like oxygen, sulfer or halogens, and most of them will react
with K in a violet manner. You will be hard pressed to find an oil that dense that in only a hydrocarbon, and I am sure that there is something that
would work, that does not react with K, but it might be pricey. Maybe a Dowtherm oil or some silicon based oil, but make sure they are stable to K
before using.
|
|