madchemist
Harmless
Posts: 3
Registered: 1-6-2004
Member Is Offline
Mood: reasonably sane
|
|
strange zinc/magnesium reaction
okay, this is my first post so if i do anything wrong please inform me.
not too long ago i tried to alloy zinc and magnesium together. Needless to say, i was sucessful but something strange occured while making it. At one
point i allowed the magnesium/zinc alloy to heat quite a bit. the reaction that ensued was really odd. the magnesium appeared to ignite as though it
were forming magnesium oxide, you know when you burn it in air, the only thing was that both the zinc and magnesium ignited and i was left with a
yellow powder of some sort. does anyone know what this is because, i have no idea.
|
|
I am a fish
undersea enforcer
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 600
Registered: 16-1-2003
Location: Bath, United Kingdom
Member Is Offline
Mood: Ichthyoidal
|
|
Did the yellow colour fade as the mixture cooled down? If so, this is due to zinc oxide. It is white when at room temperature, but yellow when hot
(due to a solid state phase transition).
1f `/0u (4|\\| |234d 7|-|15, `/0u |234||`/ |\\|33d 70 937 0u7 /\\/\\0|23.
|
|
madchemist
Harmless
Posts: 3
Registered: 1-6-2004
Member Is Offline
Mood: reasonably sane
|
|
The yellow color didn't fade or as far as i can recall. I'm pretty sure it stayed.
I would suggest others to try this little experiment, it doesn't take too long.
|
|
Esplosivo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
Quote: |
I would suggest others to try this little experiment, it doesn't take too long.
|
I am pretty sure that quite a number of us here are not able to melt magnesium at a temp of 650 deg celcius and with an inert medium
Theory guides, experiment decides.
|
|
FrankRizzo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 203
Registered: 9-2-2004
Member Is Offline
Mood: No Mood
|
|
There is really no need for an inert atmosphere when doing this experiment. Back in high school chemistry, a buddy and I did the same thing using a
bunsen burner and ceramic crucible. It's actually quite neat. If you heat the mixture to it's ignition point, it burns with a most lovely
pale-blue flame (zinc), and sends streamers of zinc oxide into the air above. The magnesium will ignite too in little "blisters" as the MgO
coating is pierced through. As to the yellow powder, I got the same stuff but didn't question as to what it was.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Like magnesium, zinc will burn in air if you get it hot enough. Burning Mg is presumably hot enough to ignite the zinc
The fumes from burning Zn are not good for you, so don't do this indoors.
My best guess for the yellow colour is the preseence of impurities (probably iron).
[Edited on 19-6-2004 by unionised]
|
|
Esplosivo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
As an impurity I would mention lead. Lead (II) Oxide is yellow (when cold). If heated the yellow PbO turns red so this can be used to test for this
hypothesis if anyone does carry out this reaction. (The red colour turns back to yellow when PbO is left to cool again)
Theory guides, experiment decides.
|
|
tantan
Harmless
Posts: 12
Registered: 15-6-2004
Member Is Offline
Mood: No Mood
|
|
From http://www.du.edu/~jcalvert/phys/zinc.htm
"If zinc oxide is breathed, the strange nervous
malady "oxide shakes" seems to result."
|
|
axehandle
Free Radical
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Quote: |
"If zinc oxide is breathed, the strange nervous
malady "oxide shakes" seems to result."
|
This would certainly explain my condition today, or perhaps it was the beer...
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
The thermochromism of lead oxide probably only works well for fairly pure samples.
[Edited on 21-6-2004 by unionised]
|
|