Electrical purification of clays
I just recently recalled my only venture into electrochemistry that was an unqualified success:
When I was seven years old, I was at my grandparents' house during Christmas vacation and my uncle, who is a soil scientist, was there too. He
showed me something that I found fascinating: adding some thick mud from the ground to water and then applying DC current caused a very silky,
fine-textured clay to accumulate on the cathode, from which it could be periodically scraped. I accumulated a film canister full of superfine clay
this way, which I still have stored somewhere.
According to the brief web-reading I just did, clays often are structured such that they have a net negative charge that is balanced out by other ions
around them. Under the influence of electricity, I guess those ions and the clays go their separate ways.
I can't think of any particularly "mad" uses for this technique, but it seemed (and seems) almost magical that such a simple procedure
can separate in such purity one component from a mixture of mud, organic debris, pebbles, sand, etc. If you ever have a chance to entice young
children with the wonders of science and technology, I think this is a worthy alternative to the usual water-splitting electrolysis demonstration.
PGP Key and corresponding e-mail address
|
|
kryss
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 77
Registered: 11-7-2003
Location: N Ireland
Member Is Offline
Mood: No Mood
|
|
I know certainly here our clays have loads of Iron in them - if you want to get rich work out a way of seperating the Iron and alumina out from them -
lots of people have tried unsuccessfully.
|
|
Cyrus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 397
Registered: 24-4-2004
Location: Ancient Persia
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by Polverone
Under the influence of electricity, I guess those ions and the clays go their separate ways.
|
Pardon me if this is a ridiculously stupid idea, and I have a feeling it is, but if all the positive ions went to one side, and the negatively charged
clay went to the other side, and you put the clay in a bottle, wouldn't you have a net negative charge in the bottle? I thought that the solution would tend to equalize the charges... some positive
ions should stay near the clay.
So if you tried the same thing with NaCl, and partitioned off the negative side of the cell, and got rid of the water, you would have a bunch of Na+?
Is that even possible?
Ok, I realize that the clay molecules are much larger per charge and so the charge is less important, but still, this seems weird.
|
|
Marvin
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 995
Registered: 13-10-2002
Member Is Offline
Mood: No Mood
|
|
Locally things will always be balenced. So seperating NaCl, the Na+ and the Cl- move apart, but the Na+ is locally balenced by OH-, and the Cl- is
balenced by the H+. The solvent alowing you to do the electrolysis has to do this, or it wouldnt be ionising.
|
|
Cyrus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 397
Registered: 24-4-2004
Location: Ancient Persia
Member Is Offline
Mood: No Mood
|
|
50 posts! Now I'm Dangerous!
Marvin, the H+ and the OH- you speak of, do the come from the autoionization of water or from electrolysis?
If they are from autoionization, then you could easily "overload" them with Na+ and Cl- ions,
if they are from electrolysis, what if you used a voltage that was not large enough to break down water? Would no ions flow anywhere, even though
they are being attracted to the anode/cathode?
|
|
notagod
Harmless
Posts: 21
Registered: 23-10-2002
Location: Sunny Scandinavia
Member Is Offline
Mood: No Mood
|
|
Hm. It would be great if one could get the gallium out of the clay instead. Perhaps it is concentrated in your "superfine clay". Not that
there is much to begin with.
|
|