Helo, i made some silver nitrate from jewellery 92,5% Ag, the whole solution was green , i evaporate , pracipatates out silver nitrate impure with
copper nitrate, i filtrated this , grren powder sometimes white , and made aqueous solution and add some copper plates to make pure silver, i must
washed too little my silver but next reacting with 40% HNO3 gave much lighter green solution, this wet powder i want to dry more quickly in heating
mantle but when i start heat my dish with "wet" AgNO3 it started to turn strong green colour, what's wrong with this chemical ? i must dry this in
dessicant or one more make silver , wash more carefully and than make "white" powder AgNO3 ?
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Green generally is from copper. Take the crude AgNO3, dry, then fuse in a ceramic container at 250 to 350 C, with stirring. Copper nitrate decomposes
at that temperature, AgNO3 does not until 440 C or thereabouts. Cool, dissolve in distilled/deionised water, filter to remove CuO. Repeat if the
solution has a blue tint.
Alternative is to ppt the silver as AgCl, wash with dilute HCl, reduce the AgCl with one of a number of reductants.
Use the search engine as this topic has been covered a number of times before.
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
i think you should've melted the the silver you got when you added the copper plates. the blue color you got probably would've burned up. i'm
surprised the silver wasnt pure enough, i always add table salt to the nitrated sterling when its all dissolved and watch it turn white then add hcl
acid and drop zinc from a penny in the mix. the black sponge will also have traces of green color when dried but will burn up before the silver sponge
melts. but i believe the method you used should yield cleaner silver.i think you just had a little copper nitrate in your silver fibers and wouldnt
have survived a torch because it was not in a metallic state.
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
If you started from sterling, you can boil it with sodium formate to give you 99,99 fine silver.
Or precipitate copper as cement, rinse the silver crystal well, and redissolve it, then precipitate with base and add sugar.
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
mario840
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 20-1-2010
Member Is Offline
Mood: No Mood
|
|
After 2 times "getting" out silver from solution AgNO3 with copper plates , and once recrystallization from water and drying over P2O5 (NOT AIR IT
TOOk FOREVER In MY CASE) i got pure product, thanks for any advice
|
|
spotlightman1234
Harmless
Posts: 17
Registered: 16-4-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by not_important ![](images/xpblue/lastpost.gif) | Green generally is from copper. Take the crude AgNO3, dry, then fuse in a ceramic container at 250 to 350 C, with stirring. Copper nitrate decomposes
at that temperature, AgNO3 does not until 440 C or thereabouts. Cool, dissolve in distilled/deionised water, filter to remove CuO. Repeat if the
solution has a blue tint.
Alternative is to ppt the silver as AgCl, wash with dilute HCl, reduce the AgCl with one of a number of reductants.
Use the search engine as this topic has been covered a number of times before.
| Wouldn't the silver nitrate also decompose to silver metal, nitrogen dioxide, and oxygen? EDIT: oops the
decomp temperature of AgNO3 is 444C. Never mind.
[Edited on 20-7-2011 by spotlightman1234]
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
Just a thought, but if you're using jewelry and getting a green color, it's probably from nickel, since that's a common jewelry alloying agent. If
copper was the contaminant, you'd be getting more of a blue color:
Copper nitrate vs. Nickel nitrate
Of course, there's a good chance you have both and your salt is a blue-green color.
[Edited on 7/21/11 by Melgar]
|
|
mario840
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 20-1-2010
Member Is Offline
Mood: No Mood
|
|
I tried many methods purify , over and over i waste about 4-5 g silver but now i know that best route is
silver/some crap (copper,nickel etc.) + HNO3 ----> silver nitrate (and crap) ------->filter and dissolve in water + NaCl(aq) -------> silver
chloride + NaOH + glucose --------> pure silver
from that silver , silver nitrate is white "snow", very pure, no waste of copper, high yield, to all who want silver refining this is for me best
method, tested over 3 times
|
|
annaandherdad
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 387
Registered: 17-9-2011
Member Is Offline
Mood: No Mood
|
|
Purifying sterling silver
Quote: Originally posted by mario840 ![](images/xpblue/lastpost.gif) | I tried many methods purify , over and over i waste about 4-5 g silver but now i know that best route is
silver/some crap (copper,nickel etc.) + HNO3 ----> silver nitrate (and crap) ------->filter and dissolve in water + NaCl(aq) -------> silver
chloride + NaOH + glucose --------> pure silver
from that silver , silver nitrate is white "snow", very pure, no waste of copper, high yield, to all who want silver refining this is for me best
method, tested over 3 times |
I agree, I've been experimenting with purifying sterling silver for several months, only recently learned about the existence of this forum. To make
a long story short, I agree that this is the best method.
One method I tried was to dissolve the sterling in HNO3, getting a blue solution of presumably AgNO3 and Cu(NO3)2, then reducing the AgNO3 with Cu
metal (I used household wire), making sure that the wire didn't completely dissolve to avoid small pieces of copper in the mix. Then filter and wash
the (beautiful) collection of silver crystals that result.
Unfortunately, when I dissolved this a second time in HNO3, it turned out green. Very glad for the suggestions here that that may be nickel, I was
wondering because copper would have been blue. Whatever it is, it is some contaminant that came out of the solution when the copper wire was added.
Not sure how this could come about, can copper reduce nickel ions? Or could it have been contamination from the copper wire itself? Anyway, this
method failed to purify the silver.
Best approach is, dissolve sterling in HNO3, precipitate AgCl, and reduce with dextrose + NaOH.
|
|
Retard-3000
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 55
Registered: 17-11-2010
Member Is Offline
Mood: No Mood
|
|
Couldn't the last step (reducing with dextrose + NaOH) be omitted as AgCl photochemically decomposes into chlorine and silver metal?
|
|
ScienceHideout
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 391
Registered: 12-3-2011
Location: In the Source
Member Is Offline
Mood: High Spin
|
|
I did the same thing... Here's what to do-
Turn the green crystals into a blue, aqueous solution. Now add copper wire. The silver will precip. out. Dissolve the precipitated silver in nitric
acid. Presto!
hey, if you are reading this, I can't U2U, but you are always welcome to send me an email!
|
|
annaandherdad
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 387
Registered: 17-9-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Retard-3000 ![](images/xpblue/lastpost.gif) | Couldn't the last step (reducing with dextrose + NaOH) be omitted as AgCl photochemically decomposes into chlorine and silver metal?
|
Yes, but it's slow and it won't work unless the light can get to all the AgCl particles, so you'd have to stir it in the light. Even with AgBr or AgI
I think it's easier to use the dextrose reduction method.
Involves heating and stirring for 15 minutes at 70-80C in a solution of NaOH and dextrose. I have a recipe I got from a research article, will look
for the details.
After doing this I dissolved again in HNO3, no green color this time, then dried out and found the silver nitrate crystals that resulted to be fine
for silvering mirrors.
Any other SF Bay chemists?
|
|
nezza
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 324
Registered: 17-4-2011
Location: UK
Member Is Offline
Mood: phosphorescent
|
|
Quote: Originally posted by not_important ![](images/xpblue/lastpost.gif) | Green generally is from copper. Take the crude AgNO3, dry, then fuse in a ceramic container at 250 to 350 C, with stirring. Copper nitrate decomposes
at that temperature, AgNO3 does not until 440 C or thereabouts. Cool, dissolve in distilled/deionised water, filter to remove CuO. Repeat if the
solution has a blue tint. |
I have used this method before and it works fine. The difference in decomp temperature is enough to completely decompose the copper nitrate before