Pages:
1
2 |
stricnine
Harmless
Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline
Mood: Hard on... working!
|
|
good rubber solvent
Hi there!
Anyone can tell of good rubber solvent/solvents? (Just in case there is misunderstanding, I'm referring to the actual material (vulcanised cautchouc),
not condoms!).
Found out that formaldehyde works, and I remember trementine could damage rubber seriously. Pentane/hexane/heptane are also on my list.
Cheers
Stricnine
|
|
chemoleo
Biochemicus Energeticus
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
Try N-methyl pyrrolidone (NMP), butyrolactone.
Havent tested it, but NMP dissolves PVC flooring, so it might do the job with rubber, too.
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
garage chemist
chemical wizard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline
Mood: No Mood
|
|
Chloroform is also a good solvent for rubber as I found out accidentally.
If chloroform is not available, dichloromethane could be used as a substitute, the solvent properties of the two are roughly the same.
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
What exactly are you trying to do here? Are you after a solution of rubber in some solvent or are you just trying to get rid of some pesky rubber in
an annoying place? If you want the latter, nitric acid might be worth a try.
|
|
stricnine
Harmless
Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline
Mood: Hard on... working!
|
|
Yeah, acqua regia is my favourite, but I want to partially dissolve rubber to more or less get a solution of it - but agaion not dissolve it
completely
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
There are hundreds of different kinds of rubber from natural rubber to Kalrez (perfluoroelastomer). The kind of rubber will highly influence the
selection of solvent. Please be more specific.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
stricnine
Harmless
Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline
Mood: Hard on... working!
|
|
It is simple rubber: 'ol natural vulcanised latex or SBR = car tyres broken down into chips. There ain´t no fluorine as far as I know. That's why I
mentioned at the beginning "vulcanised caoutchouc".
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
I missed your reference to cautchouc. I guess I am just too used to questions being asked in English on this forum.
My reference says that "oil, gasoline, kerosene, benzene, toluene, halogenated solvents, and diester lubes" will all attack SBR. I don't know which
would be a good solvent, however.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
kazaa81
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 368
Registered: 30-4-2004
Member Is Offline
Mood: ok
|
|
Maybe phosphorous oxychloride will work...
If I remember right, it was used in war first of using blistering agents (or similar) to damage the rubber of gas masks
|
|
NERV
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 152
Registered: 22-9-2002
Location: USA
Member Is Offline
Mood: Fluorinated
|
|
I personally wouldn’t use POCl3 as it is fairly hard to come by, and it’s defiantly not an armature chemist friendly compound. Plus a quick google
search didn’t yield anything about it being able to dissolve rubber although I may be wrong about that.
Vir sapit qui pauca loquitur.
|
|
stricnine
Harmless
Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline
Mood: Hard on... working!
|
|
I will be trying with Thioglycolate - permanent hair waving disulphide bond braeaker.
I will report on the results.
Keep on supporting!!
Stricnine
I am getting old. I used to push it aside with one hand... now I need both!
|
|
franklyn
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline
Mood: No Mood
|
|
US patent 4465535
Adhering Cured polymers or Prepolymers
To High Natural Rubber Elastomer
Reports that 1,2-Dichloroethane preps the surface well.
.
|
|
aonomus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 361
Registered: 18-10-2009
Location: Toronto, Canada
Member Is Offline
Mood: Refluxing
|
|
I've recently learned the hard way, that toluene over 24h does indeed make suba-seal septa swell and soften into sticky messes.
|
|
The WiZard is In
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1617
Registered: 3-4-2010
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by aonomus ![](images/xpblue/lastpost.gif) | I've recently learned the hard way, that toluene over 24h does indeed make suba-seal septa swell and soften into sticky messes.
|
----
Stamp collectors use toluene to remove glue.
|
|
JohnWW
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
Halocarbon solvents like CCl4, CHCl3, CH2Cl2, CH3CCl3, etc., should do the job, although they are mostly more expen$ive and may be liver toxins, and
have largely gone out of favor for damaging the ozone layer when their vapors are released to the atmosphere.
|
|
Vogelzang
Banned
Posts: 662
Registered: 26-4-2008
Member Is Offline
Mood: No Mood
|
|
Perchloroethylene (tetrachloroethylene) is used as a dry cleaning solvent. How hard is that to get OTC, ie. not from a chemical company? Butyl
acetate is used as a solvent for rubber cement.
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
Nonflammable paint strippers can be distilled to get CH2Cl2. They're only around $20 a gallon too.
|
|
redox
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 268
Registered: 22-2-2011
Location: The Land of Milk and Honey
Member Is Offline
Mood: Chalcogenetic
|
|
Quote: Originally posted by Vogelzang ![](images/xpblue/lastpost.gif) | Perchloroethylene (tetrachloroethylene) is used as a dry cleaning solvent. How hard is that to get OTC, ie. not from a chemical company?
|
Tetrachloroethylene is sold as a grease-remover in electronics. I bought a can of it today in Home Depot for 8 dollars.
My quite small but growing Youtube Channel: http://www.youtube.com/user/RealChemLabs
Newest video: Synthesis of Chloroform
The difference between chemists and chemical engineers: Chemists use test tubes, chemical engineers use buckets.
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
is there a way to extract elemental sulfur from rubber?
|
|
redox
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 268
Registered: 22-2-2011
Location: The Land of Milk and Honey
Member Is Offline
Mood: Chalcogenetic
|
|
Why would you want to do that?
My quite small but growing Youtube Channel: http://www.youtube.com/user/RealChemLabs
Newest video: Synthesis of Chloroform
The difference between chemists and chemical engineers: Chemists use test tubes, chemical engineers use buckets.
|
|
Mr. Wizard
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
Try a search on that poopular search engine using " rubber cement thinner " and see if will give you what you need. It might be best.
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
I have rubber, but I odn't have enough sulfur.
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2692
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
It is not possible to extract sulfur from vulcanized rubber, as it is crosslinked chemically to the rubber polymer chains. You can buiy sulfur cheap
at most drugstores or agrocultural supply stores, as it kills fungus well, and is used as "snake repellent".
Toluene is a common solvent for rubber cement, which is a solution of rubber in solvent. Mixtures of Toluene, Xylene, hexanes, and such are all
used. If you want to be able to remove the solvent, like for a glue, that is a good solution. Chloronated solvents also work well, but are very
volatile and more hazardous.
NMP and other high boiling solvents will slowly dissolve rubber and many other materials, but the resultant goo is hard to do anything further with.
|
|
Panache
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
Care to rephrase that? lol
|
|
barley81
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 481
Registered: 9-5-2011
Member Is Offline
Mood: No Mood
|
|
I read somewhere that gasoline can be used to make rubber cement, but it was used with "natural rubber". I'm not sure it would dissolve vulcanized
rubber as well or at all.
|
|
Pages:
1
2 |