Si can burn ?. since silicon is has so my covalent bonds, it can burn?
and if it will burn, will it form SiO2 (sand)?
View user's profile View All Posts By User
FritzHaber
Harmless
*




Posts: 16
Registered: 14-5-2004
Location: europe
Member Is Offline

Mood: No Mood

[*] posted on 22-5-2004 at 05:06


silicone oil with high content of higher-alkylated polysiloxanes, f.e. can burn if its preheated and ignited. and yes, depending on the oxygen supply, some SiO<sub>2</sub> will be formed.


aaahh!!:) (of course, excuse me...Si burns to SiO2)

[Edited on 22-5-2004 by FritzHaber]
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 22-5-2004 at 06:13


Silicon is an element from which semiconductors are made. Silicone is a type of polymer from which huge boobs are made.
Silicon will burn in air if finely powdered. It does produce SiO2 as you thought.
View user's profile View All Posts By User
Trojen
Harmless
*




Posts: 2
Registered: 22-5-2004
Member Is Offline

Mood: No Mood

[*] posted on 22-5-2004 at 07:27
thats cool..


thanx a lot
View user's profile View All Posts By User
avtr01
Harmless
*




Posts: 19
Registered: 10-4-2004
Location: california, united states
Member Is Offline

Mood: curious i think

[*] posted on 23-5-2004 at 03:35


Now for the opposite question. How can you make silicon ingots from SiO2? I've heard that commercial manufacturers use arc-furnaces with on crystal of silicon as the "seed", but how can amateurs like us extract it?
View user's profile View All Posts By User
hodges
National Hazard
****




Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline


[*] posted on 23-5-2004 at 12:49
Making Silicon


http://www.sciencemadness.org/talk/viewthread.php?tid=2030
View user's profile View All Posts By User
avtr01
Harmless
*




Posts: 19
Registered: 10-4-2004
Location: california, united states
Member Is Offline

Mood: curious i think

[*] posted on 23-5-2004 at 23:46


I think you just provided the link for my next project :)