[*] posted on 20-4-2011 at 16:10
Heat bendable glass tubes


When I was much younger my chemistry sets came with glass tubes for connecting into rubber stoppers with holes, etc. that could be melted above a spirit burner and bent. This allowed you to start with straight tubes and get L, C, Z, etc. shapes.

I can't seem to find these glass tubes anymore, or maybe I am not using the right search term.

Can anyone suggest where I might find them?
View user's profile View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 859
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 20-4-2011 at 16:30


"Glass tubing" ?

With a bunsen burner, you can bend borosilicate as well as soda-lime tubing.




This just in: 95,5 % of the world population lives outside the USA
You should really listen to ABBA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
View user's profile View All Posts By User
bob800
Hazard to Others
***




Posts: 240
Registered: 28-7-2010
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2011 at 16:44


A google/eBay search for "Glass Tubing" as suggested by Lambda-Eyde will give you dozens of sources. For connecting to rubber stoppers, you most likely want 5mm soda lime tubing (it's easier to melt).

For cutting tubes, you'll want a triangle file to score them. This is also readily available if you do a quick search.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2011 at 17:58


The term of art used in trade is "flint glass tubing". Google brings up plenty of vendors with this search.
View user's profile View All Posts By User
Sedit
International Hazard
*****




Posts: 1939
Registered: 23-11-2008
Member Is Offline

Mood: Manic Expressive

[*] posted on 20-4-2011 at 18:15


I could possibly sell some, im getting into glass blowing and working and I am going to pick up some supplies tommorow. I normally get Boro but Sodalime is an option.




Knowledge is useless to useless people...

"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story before."~Maynard James Keenan
View user's profile View All Posts By User
Bot0nist
International Hazard
*****




Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline

Mood: Streching my cotyledons.

[*] posted on 20-4-2011 at 18:57


I go through a lot of these. If your creative you can rig up some nice DIY rigs with them, and there inexpensive. <a href="http://unitednuclear.com/index.php?main_page=product_info&cPath=25_26&products_id=301">Glass Tubing.</a>



U.T.F.S.E. and learn the joys of autodidacticism!


Don't judge each day only by the harvest you reap, but also by the seeds you sow.
View user's profile View All Posts By User
IndependentBoffin
Hazard to Others
***




Posts: 150
Registered: 15-4-2011
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2011 at 22:33


Quote: Originally posted by bob800  
A google/eBay search for "Glass Tubing" as suggested by Lambda-Eyde will give you dozens of sources. For connecting to rubber stoppers, you most likely want 5mm soda lime tubing (it's easier to melt).

For cutting tubes, you'll want a triangle file to score them. This is also readily available if you do a quick search.


Thanks guys I remembered looking on Ebay but noted that all the glass tubing on Ebay comes from one US seller.

Let's hope he stays in business for a long time!

Local UK business suppliers are selling these at rip off prices. E.g. http://www.coleparmer.co.uk/catalog/product_view.asp?sku=347...

8mm OD, 6mm ID, 1890mm long glass tubing £248 + 20% tax. Makes you wonder if it comes in a gold plated box.

Is PTFE tubing an adequate substitute for glass tubing? In the near future I will be distilling acetic anhydride at 140C and also making white fuming nitric acid.

[Edited on 21-4-2011 by IndependentBoffin]
View user's profile View All Posts By User
bbartlog
International Hazard
*****




Posts: 1139
Registered: 27-8-2009
Location: Unmoored in time
Member Is Offline

Mood: No Mood

[*] posted on 21-4-2011 at 06:09


Depending on how much you plan to use you might want to track down a wholesale supplier. I got annoyed with the markup on little bits of tubing available on ebay and elsewhere, and ordered a box containing 250 pieces of 4' long 6mm OD borosilicate glass (Corning) for a little over a hundred dollars (but I forget where... would have to run look at the box it shipped in, which I still have).
As to whether it would melt over a spirit burner though, not sure. I use a bunsen burner.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 21-4-2011 at 14:04


Quote: Originally posted by IndependentBoffin  
Local UK business suppliers are selling these at rip off prices. E.g. http://www.coleparmer.co.uk/catalog/product_view.asp?sku=347...

8mm OD, 6mm ID, 1890mm long glass tubing £248 + 20% tax. Makes you wonder if it comes in a gold plated box.
That's 189 pieces per case and the price is per case. It's still around double what you'd pay for the same thing from a dedicated glass supplier. Standard lengths are 48 inches in the US and (IIRC) 1500 mm elsewhere.
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 1-3-2017 at 02:38


Can flint glass handle thermal shock better than soda lime glass
I cant find anything on this
If I remember right themal different within borosilicate is 200f
And soda lime is 90f where can I find the properties of this glass

Flint glass compared to soda lime glass
View user's profile View All Posts By User
battoussai114
Hazard to Others
***




Posts: 235
Registered: 18-2-2015
Member Is Offline

Mood: Not bad.... Not bad.

[*] posted on 1-3-2017 at 06:08


Quote: Originally posted by symboom  
Can flint glass handle thermal shock better than soda lime glass
I cant find anything on this
If I remember right themal different within borosilicate is 200f
And soda lime is 90f where can I find the properties of this glass

Flint glass compared to soda lime glass


This nist paper has the linear coefficient of expansion of some glasses. While I had the biggests brain fart interpreting the table but it still is at least a piece of info on the material.

[Edited on 1-3-2017 by battoussai114]




Batoussai.
View user's profile View All Posts By User
highpower48
Hazard to Self
**




Posts: 98
Registered: 30-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 1-3-2017 at 10:02


For a US retailer in small quantities try Home Science Tools
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2690
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 1-3-2017 at 10:41


Flint or soda glass does NOT handle thermal stress well, that is why most labware is borosilicate, as it has a far smaller thermal expansion coefficient. But for many uses, cheap soda glass is fine, like small pieces of tubing.

If anyone is looking for borosilicate glass tubing, I have a few pieces in several diameters, and could cut them into more easily shipable lengths. I would only ask about $1 per 4' piece, but I am happy to sell small amounts, as long as I can cut them into smaller pieces, as finding 4' shipping tubes is a pain.