Decontaminating HDPE


Have a supply of HDPE that is contaminated with an organic peroxide -- probably DTBP = Di-tert-butyl peroxide. This peroxide is typically used as a cross linking agent. The peroxide has been ABSORBED by the HDPE, but has not been heated yet, so there is no cross linking reaction. I need to EXTRACT the DTBP from the HDPE to prevent cross linking when the HDPE is melted.

Any suggestions?

Thanks!
View user's profile View All Posts By User
HydroCarbon
Hazard to Self
**




Posts: 77
Registered: 7-7-2008
Location: Anytown, USA
Member Is Offline

Mood: No Mood

[*] posted on 7-4-2011 at 15:16


You could possibly try soaking it in a solvent that the peroxide is highly soluble in, and also that swells the polymer. Im thinking methylene chloride, or chloroform.
View user's profile View All Posts By User
Curious George
Harmless
*




Posts: 15
Registered: 7-4-2011
Member Is Offline

Mood: Curious

[*] posted on 8-4-2011 at 08:39


Tried Xylene, and it worked well. Problem is that xylene is too expensive. Is there any way to do this in an AQUEOUS system?

I've tried adding caustic and adding ammonia to water. They have removed "something" from the HDPE (solutions become yellow to brown), but NOT the X linking peroxide.

Also tried several household detergents, but I'm assuming not enough 'driving force' to move the "plastic soluble" organics from the HDPE to the aqueous phase.

Any suggestions? I KNOW there are some BRILLIANT people out there !
View user's profile View All Posts By User
Eclectic
National Hazard
****




Posts: 899
Registered: 14-11-2004
Member Is Offline

Mood: Obsessive

[*] posted on 8-4-2011 at 08:51


Try kerosene?
View user's profile View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 8-4-2011 at 09:18


also ethylacetate (slower)- is the reason for extracting it because you want to melt the HDPE? If you heat it will it bond to the HDPE? (2 free rads)



"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
Curious George
Harmless
*




Posts: 15
Registered: 7-4-2011
Member Is Offline

Mood: Curious

[*] posted on 8-4-2011 at 09:29


Kerosene or #2 heating oil are my next two choices. However, I'm afraid that the lack of aromaticity will prevent good extraction. Will report back...

Yes, I want to MELT the HDPE w/o triggering the crosslinking. As is, it starts to melt and then "sets up" before I can use it. I can either remove (extract) the XL agent, OR, is there some way to PREVENT IT from working?

Either way, I'd like to do this in AQUEOUS solution (or perhaps an emulsion?) if possible.

Appreciate any advice....
View user's profile View All Posts By User
mr.crow
National Hazard
****




Posts: 884
Registered: 9-9-2009
Location: Canada
Member Is Offline

Mood: 0xFF

[*] posted on 8-4-2011 at 10:28


Can't you just get new HDPE? Unless you are operating on a large scale of course



Double, double toil and trouble; Fire burn, and caldron bubble
View user's profile View All Posts By User
HydroCarbon
Hazard to Self
**




Posts: 77
Registered: 7-7-2008
Location: Anytown, USA
Member Is Offline

Mood: No Mood

[*] posted on 8-4-2011 at 13:58


I doubt you'll be able to do it with aqueous, as the solvent (water) won't be able to penetrate the polymer matrix. Heating oil and other low grade organic materials are also a bad idea as they would contaminate your polymer with the non-volatile contaminants that are present.

One thing you may want to try is grinding the polymer to a fine powder; then you may even be able to extract the peroxide with an aqueous solution, or at least a low amount of clean solvent.
View user's profile View All Posts By User