Silver cleaner?
I have this el-cheapo silver cleaner I got at flea market and its totally unlabeled and its been dyed hot pink.
When used to clean tarnished silver (Ag2S), it gives off H2S (or maybe its SO2 but Ive never smelled that before so Im not sure, but either way, Im
sure its a sulfurous gas). However, sitting on its own in the bottle, it reacts strongly with air - enough to collapse parts of the plastic container
its in due to the vacuum created! As it sits on its own, it also makes offwhite coloured pelletlike precipitate, presumably from reacting with the
air? The liquid also oxidizes stainless steel, copper and aluminum ![:o](./images/smilies/shocked.gif)
Does anyone have an idea what this could be or any interesting ways to abuse it?
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
I am a fish
undersea enforcer
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 600
Registered: 16-1-2003
Location: Bath, United Kingdom
Member Is Offline
Mood: Ichthyoidal
|
|
I've seen silver cleaners that are acidified solutions of thiocarbamide (AKA thiourea). Be careful, as this is carcinogenic.
I have never actually bought such products, as pure thiourea is available for a much lower price from photographic suppliers.
[Edited on 3-5-2004 by I am a fish]
1f `/0u (4|\\| |234d 7|-|15, `/0u |234||`/ |\\|33d 70 937 0u7 /\\/\\0|23.
|
|
darkflame89
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
Ha, i have seen such silver cleaners too in Singapore. Usually, the label, those in the DIY shops, states that it contains HCl. I think your bottle
contains a fair amt. of HCl. As such when this dilute acid reacts with silver sulfide, i think hydrogen sulfide is given off.
Ignis ubique latet, naturam amplectitur omnem.
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Would acidified thiourea react with air to make beige granules? Unless.... its reacting with the plastic container it came in ![:o](./images/smilies/shocked.gif)
edit: Ive searched far and wide and I cant seem to find any info on silver cleaners that react with air on their own ![:mad:](./images/smilies/mad.gif)
[Edited on 4-5-2004 by Saerynide]
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
Esplosivo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
The beige granules could be due to some polymerization of some sort. The beige colour probably coming from salts present to dye the solution.
Try mixing some of this 'xilver cleaner' with sodium carbonate/hydrogen carbonate. If efferevescence occurs it's acidic. You could also
judge the degree of acidity by the rate of CO2 gas given off, but thats just basic. Nothing near to quantitative analysis ![:P](./images/smilies/tongue.gif)
Anyway, I cannot possibly imagine how this cleaner can react with air, being an acid. IF its acidic it maybe could be sulphuric acid which absorbs
moisture from the air, but that is highly improbable since the acid would be already dilute. It couls be some form of an alkaline solution like KOH
which absorbs CO2 from the air. I've had bottles of KOH soln seal up so strongly that they could not be opened up.
Theory guides, experiment decides.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
If it were a strong base and trapped all the CO2 from the air in the bottle then the pressure would fall. There is about 300 ppm of CO2 in the air so
the pressure would fall by about 0.004 PSI. I really don't think that would stop you opening the bottle.![;)](./images/smilies/wink.gif)
Given that acidified thiourea is used as a silver cleaner and that it isn't stable (hydrolysis to ammonia CO2 and H2S) and given that H2S will
slowly reduce oxygen (thereby reducing the volume) and form sulphur (a precipitate), I think we could do worse han to assume that Saerynide's
stuff is acidified thiourea.
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Now that you've mentioned it, those granules do look like sulfur Ive
been pondering for so long what that hot pink crap was. Finally an answer, thanks guys
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
darkflame89
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
Sulfur, pink? Am i missing something here?
Ignis ubique latet, naturam amplectitur omnem.
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Its been dyed pink
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
darkflame89
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
Any pics to show this?
Ignis ubique latet, naturam amplectitur omnem.
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
The yellow stuff is the sulfur:
![](http://www.sciencemadness.org/scipics/silver_cleaner.JPG)
Edit: Oops forgot the pic ![:D](./images/smilies/biggrin.gif)
[Edited on 10-5-2004 by Saerynide]
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
axehandle
Free Radical
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Looks exactly like sulfur.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
darkflame89
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
Oh boy, now we can get sulfur by just buying tons of this! Then i do not have to worry so much about finding a sulphur source. ( haha, you know what i
am ranting about. I must have gone crazy over making strong acids at home)
Where do you buy that? I have got to buy 10 bottles of it![:D](./images/smilies/biggrin.gif)