Hotblack
The pursuit of the “Ultimate Black” (a substance that can absorb all visible or non-visible light) has consumed many a scientist’s life. A
recent major breakthrough in the field was documented in a recent edition of “NewScientist” magazine; it says basically that the new ultimat black
has been found, and it is 1000 times more black than any previous ultimate black.
The procedure quoted for making it is surprisingly simple. Alloy 6% Phosphorus with 94% nickel, and then etch with Nitric Acid until (really, really,
reeeeaaally) black. The alloy proportions are quite important, as a little over, or a little under results in a very different product.
How to alloy a reactive substance like phosphorus? One would have to do so in an inert atmosphere I guess, although suggestions are welcome.
Caveat Orator
|
|
Blind Angel
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 845
Registered: 24-11-2002
Location: Québec
Member Is Offline
Mood: Meh!
|
|
There is theNewScientist Article
Quote: |
In the first stage, an object to be blackened is immersed for five hours in a solution of nickel sulphate and sodium hypophosphite. This produces a
nickel and phosphorus coating containing between five and seven per cent phosphorus. Then the surface is etched with nitric acid to produce the
super-black surface structure.
|
No mesure though, someone will need to try it
Quote: |
But the super-black alloy is quite fragile and can easily be scratched.
|
![:(](./images/smilies/sad.gif)
I requested the document on NPL, will give you news if i receive it
|
|
Nick F
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 439
Registered: 7-9-2002
Member Is Offline
Mood: No Mood
|
|
Silicon.
Zapping silicon crystals with the right sort of laser light also makes a very black black, although I'm not sure how it compares with this etched
nickel. When viewed with an electron microscope, the zapped silicon looks like a forest of regularly arranged, thin spikes. Light gets reflected down
the gaps in between the spikes many many times, and is absorbed. It was thought that if the surface could be produced cheaply and quickly that it
could lead to much more efficient solar cells.
What's nice about this nickel process is that it seems very easy - I thought we might have to add ultra-pure phosphorus to molten ultra-pure
nickel under argon or something...
|
|
Ramiel
Vicious like a ferret
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 484
Registered: 19-8-2002
Location: Room at the Back, Australia
Member Is Offline
Mood: Semi-demented
|
|
yea, that's my bad; I had only read the article in brief in the magazine. The article does say however, that this method makes a black more than
1000 times blacker than previous blacks. (boy could that be mis-quoted!)
|
|
Organikum
resurrected
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2336
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
A true challenge for the washing powder industry!
|
|
Ramiel
Vicious like a ferret
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 484
Registered: 19-8-2002
Location: Room at the Back, Australia
Member Is Offline
Mood: Semi-demented
|
|
so,
"an object to be blackened is immersed for five hours in a solution of nickel sulphate and sodium hypophosphite"
"bubbling a shiny metal plate in nitric acid for a few seconds"
on furthur searching, i found that the substrate can be plastic, ceramic, metallic or glass.
what concentration and ratio of composition is the solution?
what concentration is the nitric acid?
I'll see what NaPO<sub>3</sub> i can get a hold of and try this out.
Caveat Orator
|
|
axehandle
Free Radical
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
This could be a cheap way to harness the Sun's energy, with 100% absorption. Very interesting.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
Tacho
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 582
Registered: 5-12-2003
Member Is Offline
Mood: No Mood
|
|
There was some discussion about this in the “Ni from coins” thread:
http://www.sciencemadness.org/talk/viewthread.php?tid=534
From the formula given, it is pretty clear to me that they do electroless nickel plating on some surface and then etch it with nitric acid.
As I posted there, this is a description of electroless deposition of nickel:
http://www.ias.ac.in/sadhana/Pdf2003JunAug/Pe1104.pdf
I find it a most interesting reaction. I did some crude attempts to do it. I was able to get a nickel deposit on copper and, eventually, on glass. But
etching with nitric acid didn’t make it any black.
If anybody is interested in doing it, I must warn that there are regulations on the sale of sodium hypophosphite that are, I believe, quite
international.
|
|
Ramiel
Vicious like a ferret
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 484
Registered: 19-8-2002
Location: Room at the Back, Australia
Member Is Offline
Mood: Semi-demented
|
|
...to him that linketh in prosperity, Peace be both to thee...
<html>Here is the related press release published by the UK National Physics Laboratory - <a
href="http://www.npl.co.uk/press_centre/releases/2003/pr-07.pdf">link</a>
<i>Richard J. C. Brown , Paul J. Brewer and Martin J. T. Milton</i>, "The physical and chemical properties of electroless
nickel–phosphorus alloys and low reflectance nickel–phosphorus black surfaces", Journal Materials Chemistry, 2002, Volume 12, Issue 9, Pages
2749 to 2754 - <a href="http://www.rsc.org/CFmuscat/intermediate_abstract.cfm?FURL=/ej/JM/2002/b204483h.PDF">link</a>
^^for those of you who may have access to the JMC [lucky bastards], this will answer many questions methinks.
Edit: Can someone* tell me if the concentration of NaH<sub>2</sub>PO<sub>2</sub> is important in the disproportionation**
which occurs on the substrate*** according to this reaction?
3.H<sub>2</sub>PO<sub>2</sub><sup>-</sup> =(ads)=> 2.P<sub>(s)</sub> +
H<sub>2</sub>PO<sub>3</sub><sup>-</sup> + H<sub>2</sub>O + 2.OH
oh, and the nitric needs to be strong enough to oxidize the Ni to NiO... just a little tidbit i thought I'd share with you all.
<sub>
* Smarter than me
** My spelling sucks... bite me
*** Is this the correct term? read above.
</sub>
[Edited on 17-5-2004 by Ramiel]