Solubility of copper nitrate in nitric acid?
Anyone have a figure for this? I've tried and failed to find it with good ol' google.
FYI its part of an experiment separating silver nitrate from copper nitrate. Silver nitrate is relatively insoluble in 68% nitric acid - confirmed
when I added more nitric to concentrated copper/silver nitrate soln and got lots of little white crystals.
Yes, its the old 'get the silver out of sterling silver' problem. I've read the other threads about this, and seen the other methods - I want to try
something a bit different.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
Hexagon
Harmless
Posts: 45
Registered: 11-5-2010
Member Is Offline
Mood: Fanf*ckingtastic
|
|
AFAIK those kind of salts are not very soluble on their corresponding acids, that's common-ion effect.
Why dont you try to remove the cupric nitrate by lixiviating it in alcohol? A quick search affords that 1 part of Cu(NO3)2 is soluble in 1 part of
alcohol at 12.5 ºC while AgNO3 is only soluble 1 part in 30 of alcohol, so there you go. If you cant afford loosing that silver, then you can leave
the solution to it's own device and light will tear silver nitrate in to silver oxide, witch can be filtered.
|
|
crazyboy
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 436
Registered: 31-1-2008
Member Is Offline
Mood: Marginally insane
|
|
Copper nitrate is extremely soluble in water IIRC not sure about nitric acid. I don't even believe it is possible to isolate in a crystalline form
from an aqueous solution. If you're trying to get the silver (something I've done in the past) just dissolve the sterling in dilute nitric acid,
filter to get the silver nitrate solution, precipitate silver with copper metal, filter and melt the silver into a small ingot and purify via
electrolysis.
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
that makes sense. you can nitrate the recovered silver again if you want silver nitrate and your copper nitrate will be in solution.
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1315
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Ok, I've just redissolved the crystals I got from adding nitric acid. There is still some blue colouring - but it is much less intense.
On a side note: I found a quick way of getting clean water - ice from inside our old freezer! Its one of those ones that doesn't auto-defrost so it
steadily builds up ice on the inside walls.
I wouldn't go the alcohol route due to the risk of forming silver fulminate.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
bahamuth
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline
Mood: Under stimulated
|
|
Okay, a writeup is at hand...
Adjust pH of your solution to something like 6, and dilute to make silver displacement by copper feasible if concentrated (le chatlier).
Watch silver metal forming after adding copper metal and mix until no more silver is formed, filter and wash thoroughly with clean water . Dissolve
silver metal in Nitric acid, basify with e.g. NAOH or KOH, add sugar (yes, regular table sugar), heat to 100 degrees Celsius in a beaker with a
watchglass on top or similar apparatus under heavy stirring for atleast 24 Hours. Semi coarse grains is produced which apparently has a very high
purity, could not produce the article as my PC is down.
Any sufficiently advanced technology is indistinguishable from magic.
|
|
Sedit
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1939
Registered: 23-11-2008
Member Is Offline
Mood: Manic Expressive
|
|
Twospoons? Did you just say clean water from a freezer? Im not sure if you have checked it yet but smell anything that has been freezer burned from
your freezer, it should assure you that water is anything but clean. It is indeed full of aromatic hydrocarbons and not worth the scaping considering
how cheep distilled or spring water is from the store. Condensation from your heater is about as clean as the ice from your freezer.
Knowledge is useless to useless people...
"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the
fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story
before."~Maynard James Keenan
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1315
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
It was the cleanest I had on hand. Not much is stored in our freezer, and it doesn't smell. Mostly I wanted to avoid chlorine.
I wouldn't trust store bought water to be any cleaner. If I want really clean water I would carbon filter then distill.
Bottled water may be cheap in your part of the world, but it costs more than petrol around here. Stupid really.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
I would add HCl to precipitate silver chloride and get copper nitrate/chloride solution.
Then I would convert AgCl to Ag and Cl. Dissolve metallic silver in nitric acid and you have silver nitrate solution.
Then precipitate copper carbonate from the copper nitrate/chloride solution and again mix that copper carbonate with nitric acid.
Solutions should be separated then
|
|
entropy51
Gone, but not forgotten
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1612
Registered: 30-5-2009
Member Is Offline
Mood: Fissile
|
|
WTF?
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
On exposure to light it decomposes to silver metal and chlorine.
|
|
TheOrbit
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 59
Registered: 4-4-2009
Location: deepth point of a black hole
Member Is Offline
Mood: manic bipolar science dis/order
|
|
Quote: |
On exposure to light it decomposes to silver metal and chlorine. |
ok and then it will be oxidized " after the reduction process " to AgO
|
|
crazyboy
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 436
Registered: 31-1-2008
Member Is Offline
Mood: Marginally insane
|
|
Bad idea. AgCl is annoying it isn't water soluble, it turns into very hard clumps that are nearly impossible to break up. Sunlight and heat only
convert the outer layerto silver, and glucose reductions are messy and inefficient.
Stick with the method I mentioned.
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
S that wont work, but
There is also maybe working method with NaOH:
Put NaOH to silver and copper nitrate solution, it will precipitate AgOH, Ag2O and Cu(OH)2.
Heat that precipitated mixture until silver oxides and hydroxides will decompose to elemental silver and Cu(OH)2 to CuO and water.
Then mix decomposed mixture with hydrochloric acid to dissolve copper oxide. Elemental silver will be left.
sodium carbonate could also be used instead of lye and maybe it is even better option due to small solubility of ag(oh)2
[Edited on 1-1-2011 by Random]
|
|
The WiZard is In
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1617
Registered: 3-4-2010
Member Is Offline
Mood: No Mood
|
|
If you can't dazzle them with your brilliance ...
boggle them with a reference.
This from —
Linke's
Solubilities Inorganic and Metal-Organic Compounds
D. Van Nostrand
1958
2 Volumes 1914 pages.
![Copper-nirate-800.jpg - 207kB](http://www.sciencemadness.org/talk/files.php?pid=197011&aid=12543)
[Edited on 1-1-2011 by The WiZard is In]
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1315
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Thanks for that. An answer to the original question!
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
Twospoons you also stated it was the old silver extraction from sterling.you got about two or three methods for that now.what is copper nitrate in
nitric acid for? what is it other than copper nitrate in nitric acid?the add hcl method method will give you silver metal and chloride if you drop
zinc in it wont it?i tried that zinc and hydrochloric acid method and watched the silverchloride turn to black silver and eventually grey mud right
before my eyes.i always threw away the left over chloride. i guess i could've evaporated it and gotten zinc chloride?
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
wait a minute, i'm confused now.. don't you still have silver and copper nitrate on your hands?
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
Quote: Originally posted by cyanureeves ![](images/xpblue/lastpost.gif) | Twospoons you also stated it was the old silver extraction from sterling.you got about two or three methods for that now.what is copper nitrate in
nitric acid for? what is it other than copper nitrate in nitric acid?the add hcl method method will give you silver metal and chloride if you drop
zinc in it wont it?i tried that zinc and hydrochloric acid method and watched the silverchloride turn to black silver and eventually grey mud right
before my eyes.i always threw away the left over chloride. i guess i could've evaporated it and gotten zinc chloride? |
Or you can precipitate zinc carbonate from that with baking soda
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
thank you. i jumped in Twospoons' thread here. o.k. now! when ever i precipitate silver chloride by adding NaCl to sterling digested in nitric acid,i
do end up with sodium nitrate, copper nitrate and a bit of chlorides as well in solution don't i? would it be possible to extract the sodium
nitrate?but unless i'm dissolving a whole tea pot i guess it would'nt amount to much.
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1315
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
The idea was to displace silver nitrate from the mixed nitrates by adding excess nitric acid. Silver nitrate solubility is ~2g in 1000ml of 68%
nitric. Looking at that ref from Wizard, copper nitrate solubilty is 10X that.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
Quote: Originally posted by cyanureeves ![](images/xpblue/lastpost.gif) | thank you. i jumped in Twospoons' thread here. o.k. now! when ever i precipitate silver chloride by adding NaCl to sterling digested in nitric acid,i
do end up with sodium nitrate, copper nitrate and a bit of chlorides as well in solution don't i? would it be possible to extract the sodium
nitrate?but unless i'm dissolving a whole tea pot i guess it would'nt amount to much. |
you will have silver chloride solid and copper/sodium nitrate solution
add some more NaHCO3, Na2CO3 or NaOH to precipitate CuCO3 or Cu(OH)2 and then you have solution of sodium nitrate
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
great! AgOH and Ag2O? heck i want those now.
|
|