redmoon
Harmless
Posts: 2
Registered: 7-12-2010
Member Is Offline
Mood: No Mood
|
|
Covering Fluxes
Hi everyone,
I need a covering flux that has a low melting point such as 200 celcius degree or less. A salt flux may be helpfull. I am looking forward your
advices.
Thanks
|
|
not_important
International Hazard
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
What is it covering? Most low MP salt mixes as based on alkali metal nitrates or hydroxides, both of which are likely to react with many metals.
At the temperature you want I suspect you'll hae to go with organics, even just plain oil.
|
|
redmoon
Harmless
Posts: 2
Registered: 7-12-2010
Member Is Offline
Mood: No Mood
|
|
i need flux to cover lead metal
|
|
Magpie
lab constructor
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
I have done fire assays on gold ore having a quartz matrix. For this assay PbO is reduced to lead which collects as a button at the bottom of the
crucible. IIRC my furnace temperature was in the vicinity of 800-900C. I used a salt (NaCl) cover as recommended by Ammen in his book "Recovery and
Refining of Precious Metals." Ammen also cites the use of borax as a cover.
melting points:
Pb................327C
NaCl.............800C
Na2B4O7.....741C
Is this relevant to what you are trying to do?
[Edited on 18-12-2010 by Magpie]
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
watson.fawkes
International Hazard
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
If it's chemically compatible with what you're doing, you could use refined
bitumen, used commercially as roofing tar and for asphalt roadbed repairs.
|
|